True Stress - True Strain Curve: Part Three

概要:

The parameters that are usually determined from the true stress - true strain curve include true stress at maximum load, true fracture stress, true fracture strain, true uniform strain, true local necking strain, strain-hardening exponent and strength coefficient.

True Stress at Maximum Load


The true stress at maximum load corresponds to the true tensile strength. For most materials necking begins at maximum load at a value of strain where the true stress equals the slope of the flow curve. Let su and eu denote the true stress and true strain at maximum load when the cross-sectional area of the specimen is Au. The ultimate tensile strength is given by

Eliminating Pmax yields

(1)


True Fracture Stress


The true fracture stress is the load at fracture divided by the cross-sectional area at fracture. This stress should be corrected for the, triaxial state of stress existing in the tensile specimen at fracture. Since the data required for this correction are often not available, true-fracture-stress values are frequently in error.

True Fracture Strain


The true fracture strain ef is the true strain based on the original area A0 and the area after fracture Af

(2)

This parameter represents the maximum true strain that the material can withstand before fracture and is analogous to the total strain to fracture of the engineering stress-strain curve. Since Eq. (3) is not valid beyond the onset of necking, it is not possible to calculate ef from measured values of ef. However, for cylindrical tensile specimens the reduction of area q is related to the true fracture strain by the relationship

(3)


True Uniform Strain


The true uniform strain eu is the true strain based only on the strain up to maximum load. It may be calculated from either the specimen cross-sectional area Au or the gage length Lu at maximum load.

Equation (3) may be used to convert conventional uniform strain to true uniform strain. The uniform strain is often useful in estimating the formability of metals from the results of a tension test.

(4)


True Local Necking Strain


The local necking strain en is the strain required to deform the specimen from maximum load to fracture.

(5)

ナレッジベース検索

検索したい語句を入力:

検索方法

全文一致
キーワード

前方一致
要約

この記事は連載記事として掲載されております。詳細を見るには下記のリンクをクリックして下さい。

Total Materia Extended Range(拡張版)には数千種の金属合金塑性域、熱処理、加工温度等における計算に必要な応力‐歪み曲線が収録されております。さまざまな歪み速度に応じた真応力、エンジニアリング応力曲線も表示されます。

簡単でしかも数秒以内でデータベースの応力‐歪み曲線を探せます。

検索対象の材料を入力して下さい。材料入力のフィールドで国/規格を指定し検索を絞る事ができます。


対象材料を選んでから応力‐歪み曲線のリンクをクリックするとデータが御覧になれます。御覧になれる応力‐歪みデータの数はリンクわきのカッコ内に表示されております。


Total Materiaデータベースの応力‐歪み曲線は規格それぞれに中立的なものでサブグループのどれが適切なリンクをクリックしてデータを見て下さい。


他の加工温度に対する応力‐歪み曲線をみることができます。

まず、決められた温度範囲内で新たな温度を’ 温度入力’ のフィールドに入力するだけで構いません。

次に計算ボタンをクリックすると新しい曲線が表示され表の数字が入力された温度に応じて表示されます。 250°Cにて入力した場合の例を御覧下さい。


Total Materiaデータベースをあなたにテスト評価を頂くために15万人以上の方が登録されている無料お試しコミュニティ-へ御招待致します。