The HPAL Process

요약:

High pressure acid leaching is becoming more and more important and the inevitable strain on natural resources continues.
Its primary purpose is the assist in the recovery of nickel from lacerite ores but can also be used for other metals such as copper and cobalt.

The economic recovery of nickel from laterite ores has been pronounced for some years and will become more critical in the future, as lateritic ores constitute most of the world’s known nickel and cobalt resources, with nickel production from sulphide deposits progressively decreasing. High-pressure acid leaching (HPAL) is being used for the recovery of nickel from nickel laterite ores, and increasingly atmospheric leaching is also being considered.

As mentioned above, major reserves of nickel are contained in laterite ores, which have traditionally been treated by pyrometallurgical methods. Hydrometallurgical treatment, by direct acid leaching of the ore at temperatures above 240°C, is however an alternative treatment option for several new projects. The basic steps in the process are as follows:

There are a number of possible variations to the above basic flowsheet. Other metals, such as copper and cobalt, can also be recovered by HPAL.

On the other hand, the HPAL process is used more commonly for limonitic ores with high iron, containing low magnesium and silica. The process starts with crushing, followed by screening. In this step, it is commonly evaluated if the ore can be concentrated (beneficiated) by screening, where the enriched-silica fraction is separated from the ore.

The product from the beneficiation step is fed to the autoclave. Sulfuric acid leaching of limonite is performed at high temperatures (240-270°C) in acid resistant titanium lined autoclaves. At this temperature, equilibrium vapor pressure reaches 33-35 atm. Typical operating parameters for autoclave leaching are: pulp density of 25-35% solids, 30-90 minutes residence time, 246°C to 270°C, 200-520 kg/t of acid consumption per dry ore and 3800-5400 kPa pressure.

Iron (in the trivalent state) and aluminum follow a dissolution-precipitation path, forming solid products. Iron in the form of goethite (α FeOOH) and aluminum in the form of boehmite (AlOOH) dissolve initially to soluble ferric and aluminum sulfates respectively, according to equations (1) and (2). Gibbsite (Al(OH)3), the major aluminium phase in the limonite ore, is transformed to boehmite at around 135-155°C. Nickel and cobalt in the assumed form of oxides, dissolve according to the reactions (3) and (4) respectively and remain in the aqueous phase as sulfates.

Ferric cations hydrolyze after the dissolution of goethite, forming hematite or basic ferric sulfate, as indicated by the reaction (5) and (6). Basic ferric sulfates transform to hematite (7). Basic ferric sulfates formation depends on leaching conditions and it is favored by highly acidic environment. Higher temperature, on the other hand, favors the formation of hematite.

These reactions regenerate the acid consumed by goethite dissolution, which is one of the important advantages of the HPAL process. Aluminum cations also hydrolyze, leading to the formation of solid products. Again, most of the acid consumed by boehmite dissolution is regenerated, as shown in equations (8) and (9). The autoclave product is a hot slurry, typically at 20-25% solids, containing typically 4-6 g/l nickel, 30-60 g/l sulfuric acid, <8 g/l iron and <3 g/l aluminum.

Autoclave discharge is fed to a solid/liquid separation step. Counter-current decantation is employed in most plants. It usually involves six to seven stages of thickeners. The majority of HPAL plants burn elemental sulfur to produce sulfuric acid and the by-product steam is utilized in various unit operations.



Figure 1: High Pressure Acid Leach equipment


References

1. A.C. du Preez, M.H. Kotze: Evaluation of a versatic 10 Acid/Nicksyn Synergistic system for the recovery of nickel and cobalt from a typical lateritic leach liquor, The Southern African Institute of Mining and Metallurgy Base Metals Conference 2013, p.193-208

2. High Pressure acid leashing, SGS Minerals Services –T3 SGS 004, 2005, SGS Société Générale de Surveillance SA

3. Flavia de Melo Rezende e Sampaio Xavier: Development of technical and economical parameters affecting process selection to treat nickel laterite ores, Universidade Federal de Minas Gerais curso de pos-graduacao em engenharia netalurgica e de Minas, April 2008, Belo Horizonte Escola de Engenharia da UFMG, 2008

4. High Pressure Acid Leach and Pressure Oxidation, ALS Metallurgy, Accessed August 2015

기술 자료 검색

검색할 어구를 입력하십시오:

검색 범위

본문
키워드

머릿글
요약

Total Materia는 다양한 나라와 규격에 따른 수천개의 니켈 재질에 대한 정보를 포함하고 있습니다.

재질의 화학적 조성, 기계적 특성, 물리적 특성, 고급 물성 데이터 등의 전체적인 특성 정보들을 어디서든 검토하실 수 있습니다.

고급 검색을 이용하여, 검색 조건의 재질 리스트에서 '니켈'을 선택합니다. 검색 범위 좀 더 줄이기를 원하신다면 국가/규격과 같은 다른 조건을 지정할 수 있습니다.

검색 버튼을 클릭합니다.


선택된 정보에 부합하는 일련의 재질이 검색됩니다.


결과 리스트에서 재질을 선택하시면, 일련의 규격 사양 소그룹이 나타납니다.

여기에서 선택한 재질의 특정 특성 데이터를 검토하실 수도 있고, 강력한 상호 참조 표를 이용하여 유사 재질이나 등가 재질을 검토하는 것 또한 가능합니다.


자세한 특성 데이터를 보시려면 특성 데이터 링크를 클릭하세요.


Total Materia 데이터베이스를 사용해 보실 수 있는 기회가 있습니다. 저희는 Total Materia 무료 체험을 통해 150,000명 이상의 사용자가 이용하고 있는 커뮤니티로 귀하를 초대합니다.