Veko25Cr (PROPRIETARY) Material Properties

Material group: Ferrous Alloys / Stainless steels
Country/Standard: PROPRIETARY

Data updates

Latest Update: 2015-10
Total number of updates: 1
Update History:

Mechanical Properties


Temperature

0 - 30°C
PROPERTY / VALUE
Tensile Strength 2712 MPa view details
Rockwell Hardness (HR) 67 view details
Tensile Strength 393.3 ksi view details
Rockwell Hardness (HR) 67 view details

Physical Properties


Temperature

0 - 30°C
PROPERTY / VALUE
Modulus of Elasticity 190 — 215 GPa view details
Density 7.61 — 8.1 kg/dm³ view details
Poisson Coefficient 0.27 — 0.3 view details
Modulus of Elasticity 27.6 E+03 — 31.2 E+03 ksi view details
Density 0.275 — 0.293 lb/in³ view details
Poisson Coefficient 0.27 — 0.3 view details

Composition

CRITERIA
VALUE
UNIT
CAS NUMBER
CRITERIA
C
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7440-44-0
CRITERIA
Cr
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7440-47-3
CRITERIA
Mn
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7439-96-5
CRITERIA
Mo
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7439-98-7
CRITERIA
Nb
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7440-03-1
CRITERIA
S
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7704-34-9
CRITERIA
Si
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7440-21-3
CRITERIA
V
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7440-62-2
CRITERIA
W
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7440-33-7

Sintec HTM AG, Product Data Sheets / Available at: www.senmak.com, visited 2015

Heat Treatments

  • Annealed to 900°C, 4h. cooling rate of 12°C/h to 540°C, cooled in furnace or at still air. Hardened at 1040°C for 30 min, then heated to 1140°C for 30min, cooled in nitrogen at min. 4 bar or oil. Heat treatment 1: Hardened at 1140°C. Tempered at 450°C.