DIN 13 CrMo 4 4 Structural and constructional steels
Data updates
This material has 777 properties — only a subset is shown here.
Unlock full material properties, including detailed values across temperatures and conditions.
Free registration required • Instant access
DIN 13 CrMo 4 4 Chemical Composition
DIN 17175: 1979 / Seamless Tubes of Heat-resistant Steels - Technical Conditions of Delivery
Looking for full material performance data?
Free registration required • Instant access
DIN 13 CrMo 4 4 Physical Properties
Temperature
This material has 777 properties — only a subset is shown here.
Unlock detailed physical values across temperatures and conditions.
Free registration required • Instant access
DIN 13 CrMo 4 4 Heat Treatments
- Austenitizing: 890-950°C; Tempering: 630-740°C
- Austenizing at 890 - 950°C. Tempering at 630 - 730°C. Stress relief annealing 600 - 700°C, for t < 15 mm for at least 15 min., for 15 <= t < 30 mm at least 30 min., for t = 30 mm approx. 30 min.
DIN 13 CrMo 4 4 Mechanical Properties
Temperature
Need complete mechanical properties to make the right choice?
Get complete data on strength, hardness, fatigue, and more.
Free registration required • Instant access
DIN 13 CrMo 4 4 International Equivalent Materials
Showing 15 of 246 results.
Equivalence categories reflect chemical-composition and mechanical-property comparison — always verify suitability against the governing specification for your application.
Need the full list of 246 international equivalents?
See all 246 equivalent grades with detailed mapping by standard, producer and equivalence category.
Free registration required • Instant access
Optimize material selection for your application - Book A Demo
- 246Cross References
- 43Composition
- 164Mechanical Properties
- 52Physical Properties
- 7Heat Treatment
- -Metallography
- -Machinability
- -Stress-Strain
- -Formability
- -Fatigue
- -Fracture
- 5Creep
- 68Joints
- -Coatings
- -Dimensions
- -Tribology
- -Corrosion
- -Ageing
- -Weatherability
- -Irradiation
- 192Total Suppliers