DIN 1.6982 Cast steels

Material group: Ferrous Alloys / Cast steels
Country/Standard: Germany / DIN

Data updates

Latest Update: 2025-03
Total number of updates: 8
Update History

This material has 716 properties — only a subset is shown here.

Unlock full material properties, including detailed values across temperatures and conditions.

View Complete Material Data ›
Free registration required • Instant access

Free registration required • Instant access

DIN 1.6982 Chemical Composition

CRITERIA
VALUE
UNIT
CAS NUMBER
CRITERIA
C
VALUE
≤ 0.05
UNIT
%
CAS NUMBER
7440-44-0
CRITERIA
Cr
VALUE
12.0 – 13.5
UNIT
%
CAS NUMBER
7440-47-3
CRITERIA
Mn
VALUE
≤ 1.5
UNIT
%
CAS NUMBER
7439-96-5
CRITERIA
Mo
VALUE
val1
Full data available with free access View Complete Material Data
UNIT
%
CAS NUMBER
7439-98-7
CRITERIA
Ni
VALUE
val1
Full data available with free access View Complete Material Data
UNIT
%
CAS NUMBER
7440-02-0
CRITERIA
P
VALUE
val1
Full data available with free access View Complete Material Data
UNIT
%
CAS NUMBER
7723-14-0
CRITERIA
S
VALUE
val1
Full data available with free access View Complete Material Data
UNIT
%
CAS NUMBER
7704-34-9
CRITERIA
Si
VALUE
val1
Full data available with free access View Complete Material Data
UNIT
%
CAS NUMBER
7440-21-3

Cryogenic steel casting/steel castings having high impact strength at low temperatures - Technical delivery conditions, SEW 685 / 1989

Looking for full material performance data?

View Complete Material Data ›
Free registration required • Instant access

Free registration required • Instant access

DIN 1.6982 Physical Properties


Temperature

PROPERTY / VALUE
Modulus of Elasticity
206 GPa
Unlock full details
Full data available with free access View Complete Material Data
Density
7.7 kg/dm³
Unlock full details
Full data available with free access View Complete Material Data
Heat Capacity
val1
Full data available with free access View Complete Material Data
J/(kg∙°C)
Unlock full details
Full data available with free access View Complete Material Data

This material has 716 properties — only a subset is shown here.

Unlock detailed physical values across temperatures and conditions.

View Complete Material Data ›
Free registration required • Instant access

Free registration required • Instant access

DIN 1.6982 Heat Treatments

  • Austenitized or solutionized at 1000-1050°C, cooled in moving air or oil. Annealed at 580-620°C
  • Quenched: 1000 to 1050°C, cooled in air (for information only) and tempered: 670 to 690°C, cooled in air (for information only) and from 590 to 620°C.

DIN 1.6982 Mechanical Properties


Temperature

PROPERTY / VALUE
Yield Strength, Rp0.2
500 MPa
Unlock full details
Full data available with free access View Complete Material Data
Tensile Strength
700 — 900 MPa
Unlock full details
Full data available with free access View Complete Material Data
Elongation, A
15 %
Unlock full details
Full data available with free access View Complete Material Data
Impact Energy
val1
Full data available with free access View Complete Material Data
J
Unlock full details
Full data available with free access View Complete Material Data

Need complete mechanical properties to make the right choice?

Get complete data on strength, hardness, fatigue, and more.

View Complete Material Data ›
Free registration required • Instant access

Free registration required • Instant access

Book A Demo

Optimize material selection for your application - Book a Demo

  • 243 Cross References

  • 46 Composition
  • 35 Mechanical Properties
  • 14 Physical Properties
  • 5 Heat Treatment
  • - Metallography
  • - Machinability

  • 5 Stress-Strain
  • - Formability
  • - Fatigue
  • - Fracture
  • 5 Creep

  • - Joints
  • - Coatings
  • 136 Dimensions
  • - Tribology

  • - Corrosion
  • - Ageing
  • - Weatherability
  • - Irradiation

  • 227 Total Suppliers