30CrMo12 (European Union / EN) Material Properties
Material group:
Ferrous Alloys / Structural and constructional steels
Country/Standard:
European Union / EN
Data updates
Latest Update: 2019-07
Total number of updates: 1
Update History:
Mechanical Properties
Temperature
Physical Properties
Temperature
Coefficient of Thermal Expansion (CTE)
val1
Full data access requires a free trial.
Sign Up Free
10-6/°C
view details
Thermal Conductivity
val1
Full data access requires a free trial.
Sign Up Free
W/(m∙°C)
view details
Electrical Resistivity
val1
Full data access requires a free trial.
Sign Up Free
Ω∙mm²/m
view details
Electrical Resistivity
val1
Full data access requires a free trial.
Sign Up Free
Ω∙mm²/m
view details
Coefficient of Thermal Expansion (CTE)
val1
Full data access requires a free trial.
Sign Up Free
10-6/°F
view details
Thermal Conductivity
val1
Full data access requires a free trial.
Sign Up Free
BTU/(h∙ft∙°F)
view details
Electrical Resistivity
val1
Full data access requires a free trial.
Sign Up Free
Ω∙circular·mil/ft
view details
Electrical Resistivity
val1
Full data access requires a free trial.
Sign Up Free
Ω∙circular·mil/ft
view details
Composition
CRITERIA
VALUE
UNIT
CAS NUMBER
CRITERIA
C
VALUE
0.28 – 0.35
UNIT
%
CAS NUMBER
7440-44-0
CRITERIA
Cr
VALUE
2.80 – 3.30
UNIT
%
CAS NUMBER
7440-47-3
CRITERIA
Mn
VALUE
0.40 – 0.70
UNIT
%
CAS NUMBER
7439-96-5
CRITERIA
Mo
VALUE
val1
Full data access requires a free trial.
Sign Up Free
UNIT
%
CAS NUMBER
7439-98-7
CRITERIA
Ni
VALUE
val1
Full data access requires a free trial.
Sign Up Free
UNIT
%
CAS NUMBER
7440-02-0
CRITERIA
P
VALUE
val1
Full data access requires a free trial.
Sign Up Free
UNIT
%
CAS NUMBER
7723-14-0
CRITERIA
S
VALUE
val1
Full data access requires a free trial.
Sign Up Free
UNIT
%
CAS NUMBER
7704-34-9
CRITERIA
Si
VALUE
val1
Full data access requires a free trial.
Sign Up Free
UNIT
%
CAS NUMBER
7440-21-3
EN 3476: 2006 / Aerospace series. Steel FE-PL1501 (30CrMo12). Air melted. Softened. Forging stock. a or D ≤ 300 mm
Heat Treatments
- Hardened and tempered: 860-920°C / OQ + / >=560°C / OQ
- Hardened and tempered: 860-920°C / OQ + heating >600°C / OQ or AC.
-
98 Cross References
-
15 Composition
-
14 Mechanical Properties
-
12 Physical Properties
-
2 Heat Treatment
-
- Metallography
-
- Machinability
-
2 Stress-Strain
-
- Formability
-
- Fatigue
-
- Fracture
-
- Creep
-
- Joints
-
- Coatings
-
- Dimensions
-
- Tribology
-
- Corrosion
-
- Ageing
-
- Weatherability
-
- Irradiation
-
40 Total Suppliers