X17CrNi16-2 (Czech Republic / CSN) Material Properties
Other designations:
Material group:
Ferrous Alloys / Stainless steels
Country/Standard:
Czech Republic / CSN
Data updates
Latest Update: 2024-03
Total number of updates: 10
Update History:
2021-10
2020-03
2019-09
2019-08
2017-09
2016-10
2015-03
2015-01
2014-04
Mechanical Properties
Temperature
Physical Properties
Temperature
Coefficient of Thermal Expansion (CTE)
val1
Full data access requires a free trial.
Sign Up Free
10-6/°C
view details
Coefficient of Thermal Expansion (CTE)
val1
Full data access requires a free trial.
Sign Up Free
10-6/°C
view details
Coefficient of Thermal Expansion (CTE)
val1
Full data access requires a free trial.
Sign Up Free
10-6/°C
view details
Thermal Conductivity
val1
Full data access requires a free trial.
Sign Up Free
W/(m∙°C)
view details
Thermal Conductivity
val1
Full data access requires a free trial.
Sign Up Free
W/(m∙°C)
view details
Electrical Resistivity
val1
Full data access requires a free trial.
Sign Up Free
Ω∙mm²/m
view details
Coefficient of Thermal Expansion (CTE)
val1
Full data access requires a free trial.
Sign Up Free
10-6/°F
view details
Coefficient of Thermal Expansion (CTE)
val1
Full data access requires a free trial.
Sign Up Free
10-6/°F
view details
Coefficient of Thermal Expansion (CTE)
val1
Full data access requires a free trial.
Sign Up Free
10-6/°F
view details
Thermal Conductivity
val1
Full data access requires a free trial.
Sign Up Free
BTU/(h∙ft∙°F)
view details
Thermal Conductivity
val1
Full data access requires a free trial.
Sign Up Free
BTU/(h∙ft∙°F)
view details
Electrical Resistivity
val1
Full data access requires a free trial.
Sign Up Free
Ω∙circular·mil/ft
view details
Composition
CRITERIA
VALUE
UNIT
CAS NUMBER
CRITERIA
C
VALUE
0.12 – 0.22
UNIT
%
CAS NUMBER
7440-44-0
CRITERIA
Cr
VALUE
15.0 – 17.0
UNIT
%
CAS NUMBER
7440-47-3
CRITERIA
Mn
VALUE
≤ 1.50
UNIT
%
CAS NUMBER
7439-96-5
CRITERIA
Ni
VALUE
val1
Full data access requires a free trial.
Sign Up Free
UNIT
%
CAS NUMBER
7440-02-0
CRITERIA
P
VALUE
val1
Full data access requires a free trial.
Sign Up Free
UNIT
%
CAS NUMBER
7723-14-0
CRITERIA
S
VALUE
val1
Full data access requires a free trial.
Sign Up Free
UNIT
%
CAS NUMBER
7704-34-9
CRITERIA
Si
VALUE
val1
Full data access requires a free trial.
Sign Up Free
UNIT
%
CAS NUMBER
7440-21-3
EN 10088-1: 2023 / Stainless steels - Part 1: List of stainless steels
Heat Treatments
- A: Annealed at 600-800°C, furnace or air cooled.<br>QT800: Quenched at 1020-1080°C, oil cooled. Tempered at (580-630°C) + (550-650°C).<br>QT900: Quenched at 1020-1080°C, oil cooled. Tempered at (540-600°C) + (520-640°C).
- Hot forming: 1100-800°C, slow cooling; Annealing (+A) (Double annealing might be advisable): 680-800°C, air or furnace cooling; Quenching (+QT800): 950-1050°C, oil or air cooling; (If heat treatment is carried out in a continuous furnace, the upper part of the range specified should usually be preferred, or even exceeded); Tempering: 750-800°C + 650-700°C (In the case that the nickel is at the lower side of the range specified, a single tempering at 620 to 720°C may be sufficient); Quenching (+QT900): 950-1050°C, oil or air cooling; (If heat treatment is carried out in a continuous furnace, the upper part of the range specified should usually be preferred, or even exceeded); Tempering: 600-650°C.
-
373 Cross References
-
35 Composition
-
178 Mechanical Properties
-
52 Physical Properties
-
8 Heat Treatment
-
- Metallography
-
- Machinability
-
32 Stress-Strain
-
8 Formability
-
- Fatigue
-
- Fracture
-
- Creep
-
2 Joints
-
- Coatings
-
13 Dimensions
-
- Tribology
-
13 Corrosion
-
- Ageing
-
- Weatherability
-
- Irradiation
-
266 Total Suppliers