SEW GS-34CrNiMo6 Cast steels
Data updates
This material has 369 properties — only a subset is shown here.
Unlock full material properties, including detailed values across temperatures and conditions.
Free registration required • Instant access
SEW GS-34CrNiMo6 Chemical Composition
SEW 515: 1977 / Quenched and tempered steel casting for castings with wall thicknesses over 100 mm
Looking for full material performance data?
Free registration required • Instant access
SEW GS-34CrNiMo6 Physical Properties
Temperature
This material has 369 properties — only a subset is shown here.
Unlock detailed physical values across temperatures and conditions.
Free registration required • Instant access
SEW GS-34CrNiMo6 Heat Treatments
- Quenched at ≤ 900°C
Tempered at 600-650°C
Stress relief annealed at ≥ 570°C. This temperature must be at least 30°C below the tempering temperature and must not be below the specified minimum value
SEW GS-34CrNiMo6 Mechanical Properties
Temperature
Need complete mechanical properties to make the right choice?
Get complete data on strength, hardness, fatigue, and more.
Free registration required • Instant access
SEW GS-34CrNiMo6 International Equivalent Materials
Showing 15 of 177 results.
Equivalence categories reflect chemical-composition and mechanical-property comparison — always verify suitability against the governing specification for your application.
Need the full list of 177 international equivalents?
See all 177 equivalent grades with detailed mapping by standard, producer and equivalence category.
Free registration required • Instant access
Optimize material selection for your application - Book A Demo
- 177Cross References
- 8Composition
- 26Mechanical Properties
- 7Physical Properties
- 2Heat Treatment
- -Metallography
- -Machinability
- 6Stress-Strain
- -Formability
- -Fatigue
- -Fracture
- -Creep
- 1Joints
- -Coatings
- -Dimensions
- -Tribology
- -Corrosion
- -Ageing
- -Weatherability
- -Irradiation
- 142Total Suppliers