EN G35CrNiMo6-6 Cast steels
Material group:
Ferrous Alloys / Cast steels
Country/Standard:
European Union / EN
Data updates
Latest Update: 2015-05
Total number of updates: 1
Update History
This material has 235 properties — only a subset is shown here.
Unlock full material properties, including detailed values across temperatures and conditions.
View Complete Material Data ›
Free registration required • Instant access
Free registration required • Instant access
EN G35CrNiMo6-6 Chemical Composition
CRITERIA
VALUE
UNIT
CAS NUMBER
CRITERIA
C
VALUE
0.32 – 0.38
UNIT
%
CAS NUMBER
7440-44-0
CRITERIA
Cr
VALUE
1.40 – 1.70
UNIT
%
CAS NUMBER
7440-47-3
CRITERIA
Cu
VALUE
≤ 0.30
UNIT
%
CAS NUMBER
7440-50-8
CRITERIA
Mn
VALUE
val1
Full data available with free access
View Complete Material Data
UNIT
%
CAS NUMBER
7439-96-5
CRITERIA
Mo
VALUE
val1
Full data available with free access
View Complete Material Data
UNIT
%
CAS NUMBER
7439-98-7
CRITERIA
Ni
VALUE
val1
Full data available with free access
View Complete Material Data
UNIT
%
CAS NUMBER
7440-02-0
CRITERIA
P
VALUE
val1
Full data available with free access
View Complete Material Data
UNIT
%
CAS NUMBER
7723-14-0
CRITERIA
S
VALUE
val1
Full data available with free access
View Complete Material Data
UNIT
%
CAS NUMBER
7704-34-9
CRITERIA
Si
VALUE
val1
Full data available with free access
View Complete Material Data
UNIT
%
CAS NUMBER
7440-21-3
CRITERIA
V
VALUE
val1
Full data available with free access
View Complete Material Data
UNIT
%
CAS NUMBER
7440-62-2
EN 10293: 2015 / Steel castings for general engineering uses
Looking for full material performance data?
View Complete Material Data ›
Free registration required • Instant access
Free registration required • Instant access
This material has 235 properties — only a subset is shown here.
Unlock detailed physical values across temperatures and conditions.
View Complete Material Data ›
Free registration required • Instant access
Free registration required • Instant access
EN G35CrNiMo6-6 Heat Treatments
- Normalized (+N): 860 to 920°C, cooled in air (for information only);
(+QT1): Quenched from 860 to 920°C, cooled in liquid or air (for information only) and temperd from 600 to 650°C;
(+QT2): quenched from 860 to 920°C, cooled in liquid (for information only) and tempered from 510 to 560°C.
EN G35CrNiMo6-6 Mechanical Properties
Temperature
Yield Strength, Rp0.2
500
MPa
Unlock full details
Full data available with free access
View Complete Material Data
Tensile Strength
750 — 1050
MPa
Unlock full details
Full data available with free access
View Complete Material Data
Elongation, A
10
%
Unlock full details
Full data available with free access
View Complete Material Data
Impact Energy
Unlock full details
Full data available with free access
View Complete Material Data
Need complete mechanical properties to make the right choice?
Get complete data on strength, hardness, fatigue, and more.
View Complete Material Data ›
Book A Demo
Free registration required • Instant access
Free registration required • Instant access
Optimize material selection for your application - Book a Demo
-
109 Cross References
-
10 Composition
-
24 Mechanical Properties
-
- Physical Properties
-
1 Heat Treatment
-
- Metallography
-
- Machinability
-
- Stress-Strain
-
- Formability
-
- Fatigue
-
- Fracture
-
- Creep
-
- Joints
-
- Coatings
-
- Dimensions
-
- Tribology
-
- Corrosion
-
- Ageing
-
- Weatherability
-
- Irradiation
-
91 Total Suppliers