DIN 1.6582 Cast steels
Data updates
This material has 1402 properties — only a subset is shown here.
Unlock full material properties, including detailed values across temperatures and conditions.
Free registration required • Instant access
DIN 1.6582 Chemical Composition
EN 10269: 2013 / Steels and nickel alloys for fasteners with specified elevated and/or low temperature properties
Looking for full material performance data?
Free registration required • Instant access
DIN 1.6582 Physical Properties
Temperature
This material has 1402 properties — only a subset is shown here.
Unlock detailed physical values across temperatures and conditions.
Free registration required • Instant access
DIN 1.6582 Heat Treatments
- (+QT) Quenched: 830-860°C, cooled in water or oil; Tempered: 540-660°C.
- Quenched at ≤ 900°C
Tempered at 600-650°C
Stress relief annealed at ≥ 570°C. This temperature must be at least 30°C below the tempering temperature and must not be below the specified minimum value
DIN 1.6582 Mechanical Properties
Temperature
Need complete mechanical properties to make the right choice?
Get complete data on strength, hardness, fatigue, and more.
Free registration required • Instant access
DIN 1.6582 International Equivalent Materials
Showing 15 of 198 results.
Equivalence categories reflect chemical-composition and mechanical-property comparison — always verify suitability against the governing specification for your application.
Need the full list of 198 international equivalents?
See all 198 equivalent grades with detailed mapping by standard, producer and equivalence category.
Free registration required • Instant access
Optimize material selection for your application - Book A Demo
- 198Cross References
- 140Composition
- 474Mechanical Properties
- 63Physical Properties
- 28Heat Treatment
- 3Metallography
- -Machinability
- 96Stress-Strain
- -Formability
- 3Fatigue
- -Fracture
- -Creep
- 1Joints
- -Coatings
- 202Dimensions
- -Tribology
- -Corrosion
- -Ageing
- -Weatherability
- -Irradiation
- 194Total Suppliers