AA 6262 Alüminyum alaşım
Veri güncellemeleri
Bu malzemenin 478 özelliği vardır - burada yalnızca bir alt kümesi gösterilmektedir.
Sıcaklıklar ve koşullar genelinde ayrıntılı değerler de dahil olmak üzere tam malzeme özelliklerinin kilidini açın.
Ücretsiz kayıt gereklidir • Anında erişim
AA 6262 Kimyasal bileşim
International alloy designations and chemical composition limits for wrought aluminum and wrought aluminum alloys - Teal Sheets (2025), 2025
Tam malzeme performans verilerini mi arıyorsunuz?
Ücretsiz kayıt gereklidir • Anında erişim
AA 6262 Fiziksel özellikler
Sıcaklık
Bu malzemenin 478 özelliği vardır - burada yalnızca bir alt kümesi gösterilmektedir.
Sıcaklık ve koşullar genelinde ayrıntılı fiziksel özellik değerlerinin kilidini açın.
Ücretsiz kayıt gereklidir • Anında erişim
AA 6262 Isıl İşlem
- The times and temperatures are typical for various forms, sizes and methods of manufacture and may not exactly describe the optimum treatment for a specific item.
The nominal temperatures at which metal is heated (applies both for solution and precipitation heat treatment) should be attained as rapidly as possible and maintained ± 5°C of nominal during the time at temperature.
The time at precipitation heat treatment temperature will depend on time required for load to reach temperature. The times shown are based on rapid heating, with soaking time measured from the time the load reached within 5°C of the applicable temperature.
Material should be quenched from the solution heat-treating temperature as rapidly as possible and with minimum delay after removal from the furnace. Quenching is typically performed by immersion of wrought products in a cold water bath, although some forgings are quenched in hot-water. Quenching may be performed by alternative means such as total immersion in an aqueous polymer solution, liquefied gas, hot water, or boiling water, or by air blast or fog to minimize distortion provided samples from the material. The use of high-velocity high-volume jets of cold water is also effective for some materials.
For rolled or cold finished wire, rod and bar
Temper T4: Solution heat treated at 540°C, quenched, naturally aged. By definition, this temper designation is that which would apply after natural aging even though mechanical properties for this alloy-temper product have not been registered.
Temper T451: Solution heat treated at 540°C, quenched, naturally aged. Stress-relieved by stretching is required to produce a specified amount of permanent set subsequent to solution heat treatment. By definition, this temper designation is that which would apply after natural aging even though mechanical properties for this alloy-temper product have not been registered.
Temper T42: Solution heat treated at 540°C, quenched, naturally aged. By definition, this temper designation is that which would apply after natural aging even though mechanical properties for this alloy-temper product have not been registered.
Temper T6: Solution heat treated at 540°C, quenched, precipitation heat treated at 170° for 8 hours.
Temper T9: Solution heat treated at 540°C, quenched, precipitation heat treated at 170° for 12 hours. Cold work subsequent to precipitation heat treatment is required to attain the specified mechanical properties for this temper.
Temper T651: Solution heat treated at 540°C, quenched, precipitation heat treated at 170° for 8 hours. Stress-relieved by stretching is required to produce a specified amount of permanent set prior to any precipitation heat treatment.
Temper T62: Solution heat treated at 540°C, quenched, precipitation heat treated at 170° for 8 hours.
For extruded rod, bar, profiles and tube
Temper T4: Solution heat treated at 540°C, quenched, naturally aged. By definition, this temper designation is that which would apply after natural aging even though mechanical properties for this alloy-temper product have not been registered.
Temper T4510: Solution heat treated at 540°C, quenched, naturally aged. Stress-relieved by stretching is required to produce a specified amount of permanent set subsequent to solution heat treatment. By definition, this temper designation is that which would apply after natural aging even though mechanical properties for this alloy-temper product have not been registered.
Temper T4511: Solution heat treated at 540°C, quenched, naturally aged. Stress-relieved by stretching is required to produce a specified amount of permanent set subsequent to solution heat treatment. By definition, this temper designation is that which would apply after natural aging even though mechanical properties for this alloy-temper product have not been registered.
Temper T42: Solution heat treated at 540°C, quenched, naturally aged. By definition, this temper designation is that which would apply after natural aging even though mechanical properties for this alloy-temper product have not been registered.
Temper T6: Solution heat treated at 540°C, quenched, precipitation heat treated at 175° for 12 hours.
Temper T6510: Solution heat treated at 540°C, quenched, precipitation heat treated at 175° for 12 hours. Stress-relieved by stretching is required to produce a specified amount of permanent set prior to any precipitation heat treatment.
Temper T6511: Solution heat treated at 540°C, quenched, precipitation heat treated at 175° for 12 hours. Stress-relieved by stretching is required to produce a specified amount of permanent set prior to any precipitation heat treatment.
Temper T62: Solution heat treated at 540°C, quenched, precipitation heat treated at 175° for 12 hours.
For drawn tube
Temper T4: Solution heat treated at 540°C, quenched, naturally aged. By definition, this temper designation is that which would apply after natural aging even though mechanical properties for this alloy-temper product have not been registered.
Temper T42: Solution heat treated at 540°C, quenched, naturally aged. By definition, this temper designation is that which would apply after natural aging even though mechanical properties for this alloy-temper product have not been registered.
Temper T6: Solution heat treated at 540°C, quenched, precipitation heat treated at 170° for 8 hours.
Temper T9: Solution heat treated at 540°C, quenched, precipitation heat treated at 170° for 8 hours. Cold work subsequent to precipitation heat treatment is required to attain the specified mechanical properties for this temper.
Temper T62: Solution heat treated at 540°C, quenched, precipitation heat treated at 170° for 8 hours.
AA 6262 Mekanik özellikler
Sıcaklık
Doğru seçimi yapmak için eksiksiz mekanik özelliklere mi ihtiyacınız var?
Mukavemet, sertlik, yorulma ve daha fazlası hakkında eksiksiz verilere ulaşın.
Ücretsiz kayıt gereklidir • Anında erişim
AA 6262 Uluslararası eşdeğer malzemeler
162 sonuçtan 15 tanesi gösteriliyor.
Eşdeğerlik kategorileri, kimyasal bileşim ve mekanik özellik karşılaştırmalarını gösterir — uygulamanız için geçerli şartnameye göre uygunluğunu her zaman doğrulayın.
162 uluslararası eşdeğerin tam listesine mi ihtiyacınız var?
Standart, üretici ve eşdeğerlik kategorisine göre ayrıntılı eşleştirmeler ile tüm 162 eşdeğer kaliteleri görün.
Ücretsiz kayıt gereklidir • Anında erişim
Uygulamanız için en uygun olan malzeme seçiminizi optimize edin - Demo Rezervasyonu Yapın
- 162Çapraz Referanslar
- 26Bileşim
- 108Mekanik Özellikler
- 22Fiziksel Özellikler
- 1Isıl İşlem
- 1Metalografi
- 1İşlenebilirlik
- 19Gerilme-Gerinim
- -Şekillendirilebilirlik
- 5Yorulma
- -Kırılma
- 1Sürünmek
- -Bağlantılar
- -Kaplamalar
- -Boyutlar
- -Triboloji
- -Korozyon
- 40Yaşlanma
- -Hava şartlarına dayanıklılık
- -Radyasyon etkisi
- 92Toplam Tedarikçiler