AA 6151 Alliage d'aluminium
Mises à jour des données
Ce matériau a 275 entrées de propriétés – seul un aperçu est visible ici.
Déverrouillez l’accès aux propriétés détaillées du matériau, notamment en température et dans différentes conditions.
Inscription gratuite requise • Accès instantané
AA 6151 Composition chimique
International alloy designations and chemical composition limits for wrought aluminum and wrought aluminum alloys - Teal Sheets (2025), 2025
Vous souhaitez voir toutes les données sur ce matériau ?
Inscription gratuite requise • Accès instantané
AA 6151 Propriétés physiques
Température
Ce matériau a 275 entrées de propriétés – seul un aperçu est visible ici.
Déverrouiller l’accès aux propriétés physiques à différentes températures et conditions.
Inscription gratuite requise • Accès instantané
AA 6151 Traitement thermique
- The times and temperatures are typical for various forms, sizes and methods of manufacture and may not exactly describe the optimum treatment for a specific item.
The nominal temperatures at which metal is heated (applies both for solution and precipitation heat treatment) should be attained as rapidly as possible and maintained ± 5°C of nominal during the time at temperature.
The time at precipitation heat treatment temperature will depend on time required for load to reach temperature. The times shown are based on rapid heating, with soaking time measured from the time the load reached within 5°C of the applicable temperature.
Material should be quenched from the solution heat-treating temperature as rapidly as possible and with minimum delay after removal from the furnace. Quenching is typically performed by immersion of wrought products in a cold water bath, although some forgings are quenched in hot-water. Quenching may be performed by alternative means such as total immersion in an aqueous polymer solution, liquefied gas, hot water, or boiling water, or by air blast or fog to minimize distortion provided samples from the material. The use of high-velocity high-volume jets of cold water is also effective for some materials.
For die forgings
Temper T4: Solution heat treated at 515°C, quenched, naturally aged. By definition, this temper designation is that which would apply after natural aging even though mechanical properties for this alloy-temper product have not been registered.
Temper T6: Solution heat treated at 515°C, quenched, precipitation heat treated at 170° for 10 hours.
For rolled rings
Temper T4: Solution heat treated at 515°C, quenched, naturally aged. By definition, this temper designation is that which would apply after natural aging even though mechanical properties for this alloy-temper product have not been registered.
Temper T452: Solution heat treated at 515°C, quenched, naturally aged. Stress-relieved by 1-5 percent cold reduction subsequent to solution heat treatment. By definition, this temper designation is that which would apply after natural aging even though mechanical properties for this alloy-temper product have not been registered.
Temper T6: Solution heat treated at 515°C, quenched, precipitation heat treated at 170° for 10 hours.
Temper T652: Solution heat treated at 515°C, quenched, precipitation heat treated at 170° for 10 hours. Stress-relieved by 1-5 percent cold reduction prior to precipitation heat treatment.
AA 6151 Propriétés mécaniques
Température
Vous avez besoin des propriétés mécaniques détaillées pour faire le bon choix ?
Accédez aux données complètes de résistance, dureté, fatigue et plus encore.
Inscription gratuite requise • Accès instantané
AA 6151 Matériaux équivalents internationaux
Affichage de 15 sur 15 résultats.
Les catégories d'équivalence reflètent une comparaison de la composition chimique et des propriétés mécaniques — vérifiez toujours l'adéquation par rapport à la spécification applicable à votre utilisation.
Besoin de la liste complète des 15 équivalents internationaux ?
Consultez les 15 nuances équivalentes avec une correspondance détaillée par norme, producteur et catégorie d'équivalence.
Inscription gratuite requise • Accès instantané
Optimisez les choix de matériaux pour votre application - Réserver une démo
- 15Références croisées
- 22Composition
- 104Propriétés mécaniques
- 59Propriétés physiques
- 1Traitement thermique
- -Métallographie
- -Usinabilité
- 12Contrainte-Déformation
- -Formabilité
- 13Fatigue
- -Rupture
- 1Rampant
- -Assemblages
- -Revêtements
- -Dimensions
- -Tribologie
- 1Corrosion
- 40Vieillissement
- -Résistance aux intempéries
- -Irradiation
- 7Fournisseurs totaux