AA 6151 Aleaciones de aluminio

Grupo de materiales: Aleaciones No Ferrosas / Aleaciones de aluminio
País/Estándar: Estados Unidos / AA
Precio indicativo:

Actualizaciones de datos

Última actualización: 2020-07
Número total de actualizaciones: 5
Historial de actualizaciones
2019-05 2016-11 2016-02 2013-11

Este material cuenta con 275 propiedades — aquí solo se muestra una parte.

Accede a todas las propiedades del material, incluyendo valores detallados según temperatura y condiciones.

Ver datos completos del material ›
Se requiere registro gratuito • Acceso inmediato

Se requiere registro gratuito • Acceso inmediato

AA 6151 Composición química

Criterios
Valor
Unidad
Número CAS
Criterios
Al
Valor
Resto.
Unidad
%
Número CAS
7429-90-5
Criterios
Cr
Valor
0.15 – 0.35
Unidad
%
Número CAS
7440-47-3
Criterios
Cu
Valor
≤ 0.35
Unidad
%
Número CAS
7440-50-8
Criterios
Fe
Valor
val1
Datos completos disponibles con acceso gratuito Ver datos completos del material
Unidad
%
Número CAS
7439-89-6
Criterios
Mg
Valor
val1
Datos completos disponibles con acceso gratuito Ver datos completos del material
Unidad
%
Número CAS
7439-95-4
Criterios
Mn
Valor
val1
Datos completos disponibles con acceso gratuito Ver datos completos del material
Unidad
%
Número CAS
7439-96-5
Criterios
Other each
Valor
val1
Datos completos disponibles con acceso gratuito Ver datos completos del material
Unidad
%
Número CAS
Criterios
Other total
Valor
val1
Datos completos disponibles con acceso gratuito Ver datos completos del material
Unidad
%
Número CAS
Criterios
Si
Valor
val1
Datos completos disponibles con acceso gratuito Ver datos completos del material
Unidad
%
Número CAS
7440-21-3
Criterios
Ti
Valor
val1
Datos completos disponibles con acceso gratuito Ver datos completos del material
Unidad
%
Número CAS
7440-32-6
Criterios
Zn
Valor
val1
Datos completos disponibles con acceso gratuito Ver datos completos del material
Unidad
%
Número CAS
7440-66-6

International alloy designations and chemical composition limits for wrought aluminum and wrought aluminum alloys - Teal Sheets (2025), 2025

¿Buscas datos completos de desempeño de materiales?

Ver datos completos del material ›
Se requiere registro gratuito • Acceso inmediato

Se requiere registro gratuito • Acceso inmediato

AA 6151 Propiedades físicas


Temperatura

Propiedad/Valor
Módulo de elasticidad
69 — 79 GPa
Desbloquea todos los detalles
Datos completos disponibles con acceso gratuito Ver datos completos del material
Resistencia eléctrica
0.0319 — 0.042 Ω∙mm²/m
Desbloquea todos los detalles
Datos completos disponibles con acceso gratuito Ver datos completos del material
Densidad
val1
Datos completos disponibles con acceso gratuito Ver datos completos del material
kg/dm³
Desbloquea todos los detalles
Datos completos disponibles con acceso gratuito Ver datos completos del material
Conductividad Eléctrica
val1
Datos completos disponibles con acceso gratuito Ver datos completos del material
S/m
Desbloquea todos los detalles
Datos completos disponibles con acceso gratuito Ver datos completos del material
Temperatura de Fusión
val1
Datos completos disponibles con acceso gratuito Ver datos completos del material
°C
Desbloquea todos los detalles
Datos completos disponibles con acceso gratuito Ver datos completos del material
La conductividad térmica
163 — 205.016 W/(m∙°C)
Desbloquea todos los detalles
Datos completos disponibles con acceso gratuito Ver datos completos del material
Coeficiente de Poisson
val1
Datos completos disponibles con acceso gratuito Ver datos completos del material
Desbloquea todos los detalles
Datos completos disponibles con acceso gratuito Ver datos completos del material

Este material cuenta con 275 propiedades — aquí solo se muestra una parte.

Consulta propiedades físicas detalladas en distintas temperaturas y condiciones.

Ver datos completos del material ›
Se requiere registro gratuito • Acceso inmediato

Se requiere registro gratuito • Acceso inmediato

AA 6151 Tratamiento Térmico


  • The times and temperatures are typical for various forms, sizes and methods of manufacture and may not exactly describe the optimum treatment for a specific item.

    The nominal temperatures at which metal is heated (applies both for solution and precipitation heat treatment) should be attained as rapidly as possible and maintained ± 5°C of nominal during the time at temperature.

    The time at precipitation heat treatment temperature will depend on time required for load to reach temperature. The times shown are based on rapid heating, with soaking time measured from the time the load reached within 5°C of the applicable temperature.

    Material should be quenched from the solution heat-treating temperature as rapidly as possible and with minimum delay after removal from the furnace. Quenching is typically performed by immersion of wrought products in a cold water bath, although some forgings are quenched in hot-water. Quenching may be performed by alternative means such as total immersion in an aqueous polymer solution, liquefied gas, hot water, or boiling water, or by air blast or fog to minimize distortion provided samples from the material. The use of high-velocity high-volume jets of cold water is also effective for some materials.

    For die forgings

    Temper T4: Solution heat treated at 515°C, quenched, naturally aged. By definition, this temper designation is that which would apply after natural aging even though mechanical properties for this alloy-temper product have not been registered.

    Temper T6: Solution heat treated at 515°C, quenched, precipitation heat treated at 170° for 10 hours.

    For rolled rings

    Temper T4: Solution heat treated at 515°C, quenched, naturally aged. By definition, this temper designation is that which would apply after natural aging even though mechanical properties for this alloy-temper product have not been registered.

    Temper T452: Solution heat treated at 515°C, quenched, naturally aged. Stress-relieved by 1-5 percent cold reduction subsequent to solution heat treatment. By definition, this temper designation is that which would apply after natural aging even though mechanical properties for this alloy-temper product have not been registered.

    Temper T6: Solution heat treated at 515°C, quenched, precipitation heat treated at 170° for 10 hours.

    Temper T652: Solution heat treated at 515°C, quenched, precipitation heat treated at 170° for 10 hours. Stress-relieved by 1-5 percent cold reduction prior to precipitation heat treatment.

AA 6151 Propiedades mecánicas


Temperatura

Propiedad/Valor
Resistencia a la Tracción
≥ 290 MPa
Desbloquea todos los detalles
Datos completos disponibles con acceso gratuito Ver datos completos del material
Dureza Brinell (HB)
val1
Datos completos disponibles con acceso gratuito Ver datos completos del material
Desbloquea todos los detalles
Datos completos disponibles con acceso gratuito Ver datos completos del material
Alargamiento, A
val1
Datos completos disponibles con acceso gratuito Ver datos completos del material
%
Desbloquea todos los detalles
Datos completos disponibles con acceso gratuito Ver datos completos del material
Límite elástico, Rp0.2
val1
Datos completos disponibles con acceso gratuito Ver datos completos del material
MPa
Desbloquea todos los detalles
Datos completos disponibles con acceso gratuito Ver datos completos del material

¿Buscas información completa sobre propiedades mecánicas para tomar la mejor decisión?

Obtén información completa sobre resistencia, dureza, fatiga y más.

Ver datos completos del material ›
Se requiere registro gratuito • Acceso inmediato

Se requiere registro gratuito • Acceso inmediato

Reservar una demo

AA 6151 Materiales Internacionales Equivalentes


Mostrando 15 de 15 resultados.

Material
Estándar
País / Productor
Categoría de Equivalencia
Material
Estándar
UNS
País / Productor
Estados Unidos
Categoría de Equivalencia
Oficial
Material
Estándar
GOST
País / Productor
Rusia
Categoría de Equivalencia
Oficial
Material
Estándar
JIS
País / Productor
Japón
Categoría de Equivalencia
Oficial
Material
Estándar
GOST
País / Productor
Rusia
Categoría de Equivalencia
Oficial
Material
Estándar
AA
País / Productor
Estados Unidos
Categoría de Equivalencia
Implícito
Material
Estándar
AA
País / Productor
Estados Unidos
Categoría de Equivalencia
Implícito
Material
Estándar
ASME
País / Productor
Estados Unidos
Categoría de Equivalencia
Composición 100%
Material
Estándar
ASTM
País / Productor
Estados Unidos
Categoría de Equivalencia
Composición 100%
Material
Estándar
GB
País / Productor
China
Categoría de Equivalencia
Composición 100%
Material
Estándar
ISO
País / Productor
Internacional
Categoría de Equivalencia
Oficial
Material
Estándar
JIS
País / Productor
Japón
Categoría de Equivalencia
Oficial
Material
Estándar
SAE
País / Productor
Estados Unidos
Categoría de Equivalencia
Composición 100%
Material
Estándar
KS
País / Productor
Corea
Categoría de Equivalencia
Composición 100%
Material
Estándar
KS
País / Productor
Corea
Categoría de Equivalencia
Composición 100%
Material
Estándar
NMX
País / Productor
México
Categoría de Equivalencia
Composición 100%

Las categorías de equivalencia reflejan comparaciones de composición química y propiedades mecánicas; siempre verifique la idoneidad del material según la especificación aplicable a su aplicación.

¿Necesita la lista completa de los 15 internacionales equivalentes?

Consulte los grados 15 equivalentes con el detalle completo de correspondencias por norma, fabricante y categoría de equivalencia.

Ver Todos los Equivalentes ›
Se requiere registro gratuito • Acceso inmediato

Se requiere registro gratuito • Acceso inmediato

Reservar una demo

Optimiza la selección de materiales para tu aplicación - Reservar una demo

  • 15Referencias cruzadas

  • 22Composición
  • 104Propiedades mecánicas
  • 59Propiedades físicas
  • 1Tratamiento térmico
  • -Metalografía
  • -Maquinabilidad

  • 12Esfuerzo-Deformación
  • -Conformabilidad
  • 13Fatiga
  • -Fractura
  • 1Bicho raro

  • -Uniones
  • -Revestimientos
  • -Dimensiones
  • -Tribología

  • 1Corrosión
  • 40Envejecimiento
  • -Resistencia a la intemperie
  • -Irradiación

  • 7Proveedores Totales