B.S. TA22 Titanium Alloys
Data updates
This material has 35 properties — only a subset is shown here.
Unlock full material properties, including detailed values across temperatures and conditions.
Free registration required • Instant access
B.S. TA22 Chemical Composition
BS 2TA 22: 1973 / Specification for bar and section for machining of titanium-copper alloy (tensile strength 540-770 N/mm2)
Looking for full material performance data?
Free registration required • Instant access
B.S. TA22 Physical Properties
Temperature
This material has 35 properties — only a subset is shown here.
Unlock detailed physical values across temperatures and conditions.
Free registration required • Instant access
B.S. TA22 Heat Treatments
- The material shall be annealed as follows:
I) Heat at a temperature of 790°C ± 10°C for a time dependent on the cross section (min. 30 minutes).
II) Cool in air.
B.S. TA22 Mechanical Properties
Temperature
Need complete mechanical properties to make the right choice?
Get complete data on strength, hardness, fatigue, and more.
Free registration required • Instant access
B.S. TA22 International Equivalent Materials
Showing 9 of 9 results.
Equivalence categories reflect chemical-composition and mechanical-property comparison — always verify suitability against the governing specification for your application.
Need the full list of 9 international equivalents?
See all 9 equivalent grades with detailed mapping by standard, producer and equivalence category.
Free registration required • Instant access
Optimize material selection for your application - Book A Demo
- 9Cross References
- 4Composition
- 4Mechanical Properties
- 14Physical Properties
- 1Heat Treatment
- -Metallography
- -Machinability
- 1Stress-Strain
- -Formability
- -Fatigue
- -Fracture
- -Creep
- -Joints
- -Coatings
- -Dimensions
- -Tribology
- -Corrosion
- -Ageing
- -Weatherability
- -Irradiation
- 2Total Suppliers