TCVN 31CrMo12 Structural and constructional steels
Data updates
This material has 260 properties — only a subset is shown here.
Unlock full material properties, including detailed values across temperatures and conditions.
Free registration required • Instant access
TCVN 31CrMo12 Chemical Composition
TCVN 12142-5: 2017 / Heat treatable steels, alloy steels and free-cutting steels - Part 5: Nitriding steels
Looking for full material performance data?
Free registration required • Instant access
TCVN 31CrMo12 Physical Properties
Temperature
This material has 260 properties — only a subset is shown here.
Unlock detailed physical values across temperatures and conditions.
Free registration required • Instant access
TCVN 31CrMo12 Heat Treatments
- The base composition and the heat treatment (quenching and tempering) prior to nitriding both have an influence on the results of nitriding treatment. The tempering temperature should not be less than 50°C higher than the nitriding temperature. A difference of less than 50°C should be the subject of a special agreement.
Soft annealing at 650-700°C;
Hardening at 870-930°C (time for austenitizing as a guide: 0.5h minimum) and quenching in oil or water;
Tempering at 580-700°C (time for tempering as a guide: 1h minimum; With very large sizes, the tempering temperature may be agreed at the time of enquiry and order).;
Nitriding at 490-570°C (time for nitriding depends on the desired depth of the nitrided case).
TCVN 31CrMo12 Mechanical Properties
Temperature
Need complete mechanical properties to make the right choice?
Get complete data on strength, hardness, fatigue, and more.
Free registration required • Instant access
TCVN 31CrMo12 International Equivalent Materials
Showing 15 of 143 results.
Equivalence categories reflect chemical-composition and mechanical-property comparison — always verify suitability against the governing specification for your application.
Need the full list of 143 international equivalents?
See all 143 equivalent grades with detailed mapping by standard, producer and equivalence category.
Free registration required • Instant access
Optimize material selection for your application - Book A Demo
- 143Cross References
- 8Composition
- 21Mechanical Properties
- 3Physical Properties
- 1Heat Treatment
- -Metallography
- -Machinability
- -Stress-Strain
- -Formability
- -Fatigue
- -Fracture
- -Creep
- -Joints
- -Coatings
- -Dimensions
- -Tribology
- -Corrosion
- -Ageing
- -Weatherability
- -Irradiation
- 84Total Suppliers