PROPRIETARY Uddeholm Stavax ESR Stainless steels

Material group: Ferrous Alloys / Stainless steels
Country / Standard: PROPRIETARY

Data updates

Latest Update: 2016-05
Total number of updates: 1
Update History

This material has 36 properties — only a subset is shown here.

Unlock full material properties, including detailed values across temperatures and conditions.

View Complete Material Data ›
Free registration required • Instant access

Free registration required • Instant access

PROPRIETARY Uddeholm Stavax ESR Chemical Composition

CRITERIA
VALUE
UNIT
CAS NUMBER
CRITERIA
C
VALUE
0.38
UNIT
%
CAS NUMBER
7440-44-0
CRITERIA
Cr
VALUE
13.6
UNIT
%
CAS NUMBER
7440-47-3
CRITERIA
Mn
VALUE
0.5
UNIT
%
CAS NUMBER
7439-96-5
CRITERIA
Si
VALUE
val1
Full data available with free access View Complete Material Data
UNIT
%
CAS NUMBER
7440-21-3
CRITERIA
V
VALUE
val1
Full data available with free access View Complete Material Data
UNIT
%
CAS NUMBER
7440-62-2

Uddeholms AB, Product Data Sheets,

Looking for full material performance data?

View Complete Material Data ›
Free registration required • Instant access

Free registration required • Instant access

PROPRIETARY Uddeholm Stavax ESR Physical Properties


Temperature

PROPERTY / VALUE
Modulus of Elasticity
190 — 215 GPa
Unlock full details
Full data available with free access View Complete Material Data
Thermal Conductivity
val1
Full data available with free access View Complete Material Data
W/(m∙°C)
Unlock full details
Full data available with free access View Complete Material Data
Density
val1
Full data available with free access View Complete Material Data
kg/dm³
Unlock full details
Full data available with free access View Complete Material Data
Heat Capacity
val1
Full data available with free access View Complete Material Data
J/(kg∙°C)
Unlock full details
Full data available with free access View Complete Material Data
Poisson Coefficient
val1
Full data available with free access View Complete Material Data
Unlock full details
Full data available with free access View Complete Material Data

This material has 36 properties — only a subset is shown here.

Unlock detailed physical values across temperatures and conditions.

View Complete Material Data ›
Free registration required • Instant access

Free registration required • Instant access

PROPRIETARY Uddeholm Stavax ESR Heat Treatments


  • Soft annealing: Protect the steel and heat through to 890°C (1630°F). Then cool in the furnace at 20°C (36°F) per hour to 850°C (1560°F), then at 10°C (18°F) per hour to 700°C (1290°F), then freely in air;
    Stress-relieving: After rough machining the tool should be heated through to 650°C (1200°F), holding time 2 hr. Cool slowly to 500°C (930°F), then freely in air;
    Hardening: Preheating temperature: 600-850°C (1110-1560°F). Austenitizing temperature: 1000-1050°C (1830-1920°F), but usually 1020-1030°C (1870-1885°F).
    Quenching media: Fluidized bed or salt bath at 250-550°C (480-1020°F), then cool in air blast, Vacuum with sufficient positive pressure, High speed gas/circulating atmosphere. In order to obtain optimum properties, the cooling rate should be as fast as is concomitant with acceptable distortion. When heat treating in a vacuum furnace, a 4-5 bar overpressure is recommended. Temper immediately when the tool reaches 50-70°C (120-160°F);
    Tempering: Choose the tempering temperature according to the hardness. Temper twice with intermediate cooling to room temperature. Lowest tempering temperature 250°C (480°F), holding for minimum of 2 h.
  • Austenitizing temperature 1030°C (1890°F). Holding time 30 minutes.

PROPRIETARY Uddeholm Stavax ESR Mechanical Properties


Temperature

PROPERTY / VALUE
Tensile Strength
1420 — 1780 MPa
Unlock full details
Full data available with free access View Complete Material Data
Brinell Hardness (HB)
190
Unlock full details
Full data available with free access View Complete Material Data
Rockwell Hardness (HR)
val1
Full data available with free access View Complete Material Data
Unlock full details
Full data available with free access View Complete Material Data
Yield Strength, Rp0.2
1280 — 1360 MPa
Unlock full details
Full data available with free access View Complete Material Data

Need complete mechanical properties to make the right choice?

Get complete data on strength, hardness, fatigue, and more.

View Complete Material Data ›
Free registration required • Instant access

Free registration required • Instant access

Book A Demo

PROPRIETARY Uddeholm Stavax ESR International Equivalent Materials


Showing 1 of 3 results.

MATERIAL
STANDARD
COUNTRY / PRODUCER
EQUIVALENCE CATEGORY
MATERIAL
STANDARD
PROPRIETARY
COUNTRY / PRODUCER
EQUIVALENCE CATEGORY
Composition 100%

Equivalence categories reflect chemical-composition and mechanical-property comparison — always verify suitability against the governing specification for your application.

Need the full list of 3 international equivalents?

See all 3 equivalent grades with detailed mapping by standard, producer and equivalence category.

View All Equivalents ›
Free registration required • Instant access

Free registration required • Instant access

Book A Demo

Optimize material selection for your application - Book A Demo

  • 3Cross References

  • 5Composition
  • 7Mechanical Properties
  • 15Physical Properties
  • 3Heat Treatment
  • -Metallography
  • -Machinability

  • -Stress-Strain
  • -Formability
  • -Fatigue
  • -Fracture
  • -Creep

  • 1Joints
  • -Coatings
  • -Dimensions
  • -Tribology

  • -Corrosion
  • -Ageing
  • -Weatherability
  • -Irradiation

  • 2Total Suppliers