ASTM A 426 J84090 Structural and constructional steels
Data updates
This material has 120 properties — only a subset is shown here.
Unlock full material properties, including detailed values across temperatures and conditions.
Free registration required • Instant access
ASTM A 426 J84090 Chemical Composition
A426/A426M: 2011 / Centrifugally Cast Ferritic Alloy Steel Pipe for High-Temperature Service
Looking for full material performance data?
Free registration required • Instant access
ASTM A 426 J84090 Physical Properties
Temperature
This material has 120 properties — only a subset is shown here.
Unlock detailed physical values across temperatures and conditions.
Free registration required • Instant access
ASTM A 426 J84090 Heat Treatments
- Normalized and tempered or liquid-quenched and tempered condition. Ausenitized at 1040 – 1080 °C and tempered at 730 – 800 °C.
ASTM A 426 J84090 Mechanical Properties
Temperature
Need complete mechanical properties to make the right choice?
Get complete data on strength, hardness, fatigue, and more.
Free registration required • Instant access
ASTM A 426 J84090 International Equivalent Materials
Showing 15 of 83 results.
Equivalence categories reflect chemical-composition and mechanical-property comparison — always verify suitability against the governing specification for your application.
Need the full list of 83 international equivalents?
See all 83 equivalent grades with detailed mapping by standard, producer and equivalence category.
Free registration required • Instant access
Optimize material selection for your application - Book A Demo
- 83Cross References
- 14Composition
- 5Mechanical Properties
- 3Physical Properties
- 1Heat Treatment
- -Metallography
- -Machinability
- -Stress-Strain
- -Formability
- -Fatigue
- -Fracture
- -Creep
- -Joints
- -Coatings
- 8Dimensions
- -Tribology
- -Corrosion
- -Ageing
- -Weatherability
- -Irradiation
- 6Total Suppliers