PROPRIETARY K12 Cast irons
Data updates
This material has 147 properties — only a subset is shown here.
Unlock full material properties, including detailed values across temperatures and conditions.
Free registration required • Instant access
PROPRIETARY K12 Chemical Composition
IMS Group, Product Data Sheets,
Looking for full material performance data?
Free registration required • Instant access
PROPRIETARY K12 Heat Treatments
- Isothermal annealing at 850°C, hold for 0.5 - 1h, furnace cooling to 770°C and hold at temperature for at least 10h, cool by 10°C/h to 720°C, cooling in air. Stress relieving at 650 - 700°C, hold for 4 - 6h, furnace cooling to 300 - 350°C, cooling in air. Hardening: initial preheating to 350 - 450°C, second preheating to 750 - 850°C in salt bath at 850°C, austenitizing at 960 - 1000°C, cooling in fluid oil. Tempering at 150 - 300°C for at least 2 - 3h.
PROPRIETARY K12 Mechanical Properties
Temperature
Need complete mechanical properties to make the right choice?
Get complete data on strength, hardness, fatigue, and more.
Free registration required • Instant access
PROPRIETARY K12 International Equivalent Materials
Showing 15 of 73 results.
Equivalence categories reflect chemical-composition and mechanical-property comparison — always verify suitability against the governing specification for your application.
Need the full list of 73 international equivalents?
See all 73 equivalent grades with detailed mapping by standard, producer and equivalence category.
Free registration required • Instant access
Optimize material selection for your application - Book A Demo
- 73Cross References
- 4Composition
- 3Mechanical Properties
- -Physical Properties
- 1Heat Treatment
- -Metallography
- -Machinability
- -Stress-Strain
- -Formability
- -Fatigue
- -Fracture
- -Creep
- -Joints
- -Coatings
- -Dimensions
- -Tribology
- -Corrosion
- -Ageing
- -Weatherability
- -Irradiation