CSN 34 CrAlMo 5-10 Structural and constructional steels
Data updates
This material has 342 properties — only a subset is shown here.
Unlock full material properties, including detailed values across temperatures and conditions.
Free registration required • Instant access
CSN 34 CrAlMo 5-10 Chemical Composition
EN 10085: 2001 / Nitriding steels - Technical delivery conditions
Looking for full material performance data?
Free registration required • Instant access
CSN 34 CrAlMo 5-10 Physical Properties
Temperature
This material has 342 properties — only a subset is shown here.
Unlock detailed physical values across temperatures and conditions.
Free registration required • Instant access
CSN 34 CrAlMo 5-10 Heat Treatments
- Soft annealing: 650-750°C; Hardening: 870-930°C (0,5 h minimum), oil or water cooling; Tempering: 580-700°C (1 h minimum); Nitriding: 480-570°C.
CSN 34 CrAlMo 5-10 Mechanical Properties
Temperature
Need complete mechanical properties to make the right choice?
Get complete data on strength, hardness, fatigue, and more.
Free registration required • Instant access
CSN 34 CrAlMo 5-10 International Equivalent Materials
Showing 15 of 162 results.
Equivalence categories reflect chemical-composition and mechanical-property comparison — always verify suitability against the governing specification for your application.
Need the full list of 162 international equivalents?
See all 162 equivalent grades with detailed mapping by standard, producer and equivalence category.
Free registration required • Instant access
Optimize material selection for your application - Book A Demo
- 162Cross References
- 16Composition
- 22Mechanical Properties
- 3Physical Properties
- 5Heat Treatment
- -Metallography
- -Machinability
- -Stress-Strain
- -Formability
- 5Fatigue
- -Fracture
- -Creep
- -Joints
- -Coatings
- -Dimensions
- -Tribology
- -Corrosion
- -Ageing
- -Weatherability
- -Irradiation
- 129Total Suppliers