EN 1.6580 Structural and constructional steels
Data updates
This material has 847 properties — only a subset is shown here.
Unlock full material properties, including detailed values across temperatures and conditions.
Free registration required • Instant access
EN 1.6580 Chemical Composition
EN 10083-1: 1991 / Quenched and tempered steels - Part 1: Technical delivery conditions for special steels (includes amendment A1:1996)
Looking for full material performance data?
Free registration required • Instant access
EN 1.6580 Physical Properties
Temperature
This material has 847 properties — only a subset is shown here.
Unlock detailed physical values across temperatures and conditions.
Free registration required • Instant access
EN 1.6580 Heat Treatments
- (+QT) Quenched: 830-860°C, cooled in water or oil; Tempered: 540-660°C.
- Annealed (+A): 650-700°C Normalized (+N): 850-880°C Austenitized: 830-860°C Tempered: 540-680°C
EN 1.6580 Mechanical Properties
Temperature
Need complete mechanical properties to make the right choice?
Get complete data on strength, hardness, fatigue, and more.
Free registration required • Instant access
Optimize material selection for your application - Book a Demo
-
142 Cross References
-
84 Composition
-
207 Mechanical Properties
-
24 Physical Properties
-
23 Heat Treatment
-
6 Metallography
-
- Machinability
-
4 Stress-Strain
-
- Formability
-
12 Fatigue
-
- Fracture
-
- Creep
-
1 Joints
-
- Coatings
-
208 Dimensions
-
- Tribology
-
- Corrosion
-
- Ageing
-
- Weatherability
-
- Irradiation
-
136 Total Suppliers