C35R (European Union / EN) Material Properties
Other designations:
Material group:
Ferrous Alloys / Structural and constructional steels
Country/Standard:
European Union / EN
Data updates
Latest Update: 2024-12
Total number of updates: 6
Update History:
2019-06
2019-02
2018-10
2018-09
2018-08
Mechanical Properties
Temperature
Physical Properties
Temperature
Composition
CRITERIA
VALUE
UNIT
CAS NUMBER
CRITERIA
C
VALUE
0.32 – 0.39
UNIT
%
CAS NUMBER
7440-44-0
CRITERIA
Cr
VALUE
≤ 0.40
UNIT
%
CAS NUMBER
7440-47-3
CRITERIA
Cr+Mo+Ni
VALUE
≤ 0.63
UNIT
%
CAS NUMBER
CRITERIA
Mn
VALUE
val1
Full data access requires a free trial.
Sign Up Free
UNIT
%
CAS NUMBER
7439-96-5
CRITERIA
Mo
VALUE
val1
Full data access requires a free trial.
Sign Up Free
UNIT
%
CAS NUMBER
7439-98-7
CRITERIA
Ni
VALUE
val1
Full data access requires a free trial.
Sign Up Free
UNIT
%
CAS NUMBER
7440-02-0
CRITERIA
P
VALUE
val1
Full data access requires a free trial.
Sign Up Free
UNIT
%
CAS NUMBER
7723-14-0
CRITERIA
S
VALUE
val1
Full data access requires a free trial.
Sign Up Free
UNIT
%
CAS NUMBER
7704-34-9
CRITERIA
Si
VALUE
val1
Full data access requires a free trial.
Sign Up Free
UNIT
%
CAS NUMBER
7440-21-3
EN 10083-1: 1991 / Quenched and tempered steels - Part 1: Technical delivery conditions for special steels (includes amendment A1:1996)
Heat Treatments
- <b> Hardening: </b> 840-880°C (Temperatures at the lower end of the range are generally used for water, and those at the upper end for oil quenching; Time for austenitizing as a guide: at least 30 min.); <br> <b> Quenching agent: </b> Water or oil (Other quenching agents such as synthetic quenchants may also be used.); <br> <b> Tempering:</b> 550-660°C (Time for tempering as a guide: at least 1h.); <br> <b> End quench test austenitizing:</b> 870 ± 5°C (Time for austenitizing as a guide: 30-35 min.); <br> <b> Normalizing:</b> 860-900°C.
- Austenitizing (at least 30 min), quenching in water or oil: 840-880°C (the temperatures at the lower end of the range are generally applicable to quenching in water and those at the upper end for quenching in oil), other quenching agents such as synthetic quenchants may also be used; Tempering: 550-660°C (at least 60 min); End quench test: 870 (±5°C); Normalizing: 860-920°C, austenitizing (at least 30 min).
-
406 Cross References
-
66 Composition
-
242 Mechanical Properties
-
3 Physical Properties
-
8 Heat Treatment
-
- Metallography
-
- Machinability
-
- Stress-Strain
-
- Formability
-
10 Fatigue
-
- Fracture
-
- Creep
-
- Joints
-
- Coatings
-
6 Dimensions
-
- Tribology
-
- Corrosion
-
- Ageing
-
- Weatherability
-
- Irradiation
-
294 Total Suppliers