1.1181 (Germany / DIN) Material Properties
Other designations:
, ,
Material group:
Ferrous Alloys / Structural and constructional steels
Country/Standard:
Germany / DIN
Data updates
Latest Update: 2025-03
Total number of updates: 16
Update History:
2024-12
2024-08
2024-07
2024-05
2022-08
2021-12
2019-06
2019-01
2018-09
2018-08
2018-07
2017-10
2016-05
2015-04
2014-04
Mechanical Properties
Temperature
Physical Properties
Temperature
Dynamic Modulus of Elasticity
val1
Full data access requires a free trial.
Sign Up Free
GPa
view details
Dynamic Modulus of Elasticity
val1
Full data access requires a free trial.
Sign Up Free
GPa
view details
Dynamic Modulus of Elasticity
val1
Full data access requires a free trial.
Sign Up Free
GPa
view details
Dynamic Modulus of Elasticity
val1
Full data access requires a free trial.
Sign Up Free
GPa
view details
Coefficient of Thermal Expansion (CTE)
val1
Full data access requires a free trial.
Sign Up Free
10-6/°C
view details
Coefficient of Thermal Expansion (CTE)
val1
Full data access requires a free trial.
Sign Up Free
10-6/°C
view details
Coefficient of Thermal Expansion (CTE)
val1
Full data access requires a free trial.
Sign Up Free
10-6/°C
view details
Dynamic Modulus of Elasticity
val1
Full data access requires a free trial.
Sign Up Free
ksi
view details
Dynamic Modulus of Elasticity
val1
Full data access requires a free trial.
Sign Up Free
ksi
view details
Dynamic Modulus of Elasticity
val1
Full data access requires a free trial.
Sign Up Free
ksi
view details
Dynamic Modulus of Elasticity
val1
Full data access requires a free trial.
Sign Up Free
ksi
view details
Coefficient of Thermal Expansion (CTE)
val1
Full data access requires a free trial.
Sign Up Free
10-6/°F
view details
Coefficient of Thermal Expansion (CTE)
val1
Full data access requires a free trial.
Sign Up Free
10-6/°F
view details
Coefficient of Thermal Expansion (CTE)
val1
Full data access requires a free trial.
Sign Up Free
10-6/°F
view details
Composition
CRITERIA
VALUE
UNIT
CAS NUMBER
CRITERIA
C
VALUE
0.3200 – 0.3900
UNIT
%
CAS NUMBER
7440-44-0
CRITERIA
Mn
VALUE
0.5000 – 0.8000
UNIT
%
CAS NUMBER
7439-96-5
CRITERIA
P
VALUE
≤ 0.0350
UNIT
%
CAS NUMBER
7723-14-0
CRITERIA
S
VALUE
val1
Full data access requires a free trial.
Sign Up Free
UNIT
%
CAS NUMBER
7704-34-9
CRITERIA
Si
VALUE
val1
Full data access requires a free trial.
Sign Up Free
UNIT
%
CAS NUMBER
7440-21-3
DIN 1652-4: 1990 / Bright steel made from steel for quenching and tempering; technical delivery conditions
Heat Treatments
- (+N) Normalized: 860-900°C, cooled in air;<br />(+QT) Quenched: 840-880°C, cooled in oil or water, Tempered: 550-660°C.
- Annealed (+A): 650-700°C Normalized (+N): 860-900°C Austenitized: 840-880°C Tempered: 550-680°C
-
785 Cross References
-
139 Composition
-
637 Mechanical Properties
-
74 Physical Properties
-
19 Heat Treatment
-
4 Metallography
-
- Machinability
-
170 Stress-Strain
-
17 Formability
-
10 Fatigue
-
- Fracture
-
2 Creep
-
- Joints
-
- Coatings
-
173 Dimensions
-
- Tribology
-
- Corrosion
-
- Ageing
-
- Weatherability
-
- Irradiation
-
588 Total Suppliers