DIN C22E Structural and constructional steels
Data updates
This material has 10180 properties — only a subset is shown here.
Unlock full material properties, including detailed values across temperatures and conditions.
Free registration required • Instant access
DIN C22E Chemical Composition
EN 10132-3: 2000 / Cold rolled narrow steel strip for heat treatment - Technical delivery conditions - Part 3: Steels for quenching and tempering
Looking for full material performance data?
Free registration required • Instant access
DIN C22E Physical Properties
Temperature
This material has 10180 properties — only a subset is shown here.
Unlock detailed physical values across temperatures and conditions.
Free registration required • Instant access
DIN C22E Heat Treatments
- Annealed (+A): 650-700°C Normalized (+N): 880-920°C Austenitized: 860-900°C Tempered: 550-680°C
- Austenitizing (at least 30 min), quenching in water: 860-900°C (the temperatures at the lower end of the range are generally applicable to quenching in water and those at the upper end for quenching in oil), other quenching agents such as synthetic quenchants may also be used; Tempering: 550-660°C (at least 60 min); Normalizing: 880-940°C, austenitizing (at least 30 min).
DIN C22E Mechanical Properties
Temperature
Need complete mechanical properties to make the right choice?
Get complete data on strength, hardness, fatigue, and more.
Free registration required • Instant access
Optimize material selection for your application - Book a Demo
-
792 Cross References
-
45 Composition
-
69 Mechanical Properties
-
12 Physical Properties
-
4 Heat Treatment
-
5 Metallography
-
- Machinability
-
18 Stress-Strain
-
1 Formability
-
16 Fatigue
-
- Fracture
-
- Creep
-
83 Joints
-
- Coatings
-
10 Dimensions
-
1 Tribology
-
8491 Corrosion
-
- Ageing
-
- Weatherability
-
- Irradiation
-
633 Total Suppliers