DIN Ck 22 Structural and constructional steels
Data updates
This material has 1697 properties — only a subset is shown here.
Unlock full material properties, including detailed values across temperatures and conditions.
Free registration required • Instant access
DIN Ck 22 Chemical Composition
DIN 1652-4: 1990 / Bright steel made from steel for quenching and tempering; technical delivery conditions
Looking for full material performance data?
Free registration required • Instant access
DIN Ck 22 Physical Properties
Temperature
This material has 1697 properties — only a subset is shown here.
Unlock detailed physical values across temperatures and conditions.
Free registration required • Instant access
DIN Ck 22 Heat Treatments
- Hot working: 1100-900°C; Soft annealing: 650-700°C; Normalizing: 880-910°C; Hardening in water: 860-890°C; Hardening in oil: 870-900°C; Tempering: 550-660°C
DIN Ck 22 Mechanical Properties
Temperature
Need complete mechanical properties to make the right choice?
Get complete data on strength, hardness, fatigue, and more.
Free registration required • Instant access
DIN Ck 22 International Equivalent Materials
Showing 15 of 804 results.
Equivalence categories reflect chemical-composition and mechanical-property comparison — always verify suitability against the governing specification for your application.
Need the full list of 804 international equivalents?
See all 804 equivalent grades with detailed mapping by standard, producer and equivalence category.
Free registration required • Instant access
Optimize material selection for your application - Book A Demo
- 804Cross References
- 20Composition
- 155Mechanical Properties
- 3Physical Properties
- 3Heat Treatment
- -Metallography
- -Machinability
- 1Stress-Strain
- 1Formability
- 16Fatigue
- -Fracture
- -Creep
- 83Joints
- -Coatings
- -Dimensions
- -Tribology
- -Corrosion
- -Ageing
- -Weatherability
- -Irradiation
- 611Total Suppliers