1.0402 (Germany / DIN) Material Properties
Other designations:
Material group:
Ferrous Alloys / Structural and constructional steels
Country/Standard:
Germany / DIN
Data updates
Latest Update: 2020-12
Total number of updates: 3
Update History:
2019-06
2017-02
Mechanical Properties
Temperature
Physical Properties
Temperature
Coefficient of Thermal Expansion (CTE)
val1
Full data access requires a free trial.
Sign Up Free
10-6/°C
view details
Coefficient of Thermal Expansion (CTE)
val1
Full data access requires a free trial.
Sign Up Free
10-6/°F
view details
Composition
CRITERIA
VALUE
UNIT
CAS NUMBER
CRITERIA
C
VALUE
0.1800 – 0.2500
UNIT
%
CAS NUMBER
7440-44-0
CRITERIA
Mn
VALUE
0.3000 – 0.6000
UNIT
%
CAS NUMBER
7439-96-5
CRITERIA
P
VALUE
≤ 0.0450
UNIT
%
CAS NUMBER
7723-14-0
CRITERIA
S
VALUE
val1
Full data access requires a free trial.
Sign Up Free
UNIT
%
CAS NUMBER
7704-34-9
CRITERIA
Si
VALUE
val1
Full data access requires a free trial.
Sign Up Free
UNIT
%
CAS NUMBER
7440-21-3
DIN 1652-4: 1990 / Bright steel made from steel for quenching and tempering; technical delivery conditions
Heat Treatments
- Annealing: 650-700°C; Normalizing: 880-910°C; Hardening in water: 860-890°C; Tempering: 540-680°C
- Austenitizing (quenching in water): 860-900°C, t > 30 min. Tempering: 550-660°C, t > 60 min. Normalizing: 880-920°C, t > 30 min.
-
462 Cross References
-
38 Composition
-
164 Mechanical Properties
-
10 Physical Properties
-
5 Heat Treatment
-
- Metallography
-
- Machinability
-
71 Stress-Strain
-
22 Formability
-
11 Fatigue
-
- Fracture
-
- Creep
-
87 Joints
-
- Coatings
-
4 Dimensions
-
1 Tribology
-
8491 Corrosion
-
- Ageing
-
- Weatherability
-
- Irradiation
-