DIN 41 CrMo 4 Structural and constructional steels
Data updates
This material has 224 properties — only a subset is shown here.
Unlock full material properties, including detailed values across temperatures and conditions.
Free registration required • Instant access
DIN 41 CrMo 4 Chemical Composition
DIN 17212: 1972 / Flame and Induction Hardening Steels; Quality Specifications
Looking for full material performance data?
Free registration required • Instant access
DIN 41 CrMo 4 Physical Properties
Temperature
This material has 224 properties — only a subset is shown here.
Unlock detailed physical values across temperatures and conditions.
Free registration required • Instant access
DIN 41 CrMo 4 Heat Treatments
- Hot working: 1050-850°C; Softening: 680-720°C; Normalizing: 840-880°C; Hardening in water: 820-850°C; Hardening in oil: 830-860°C; Tempering: 540-680°C
DIN 41 CrMo 4 Mechanical Properties
Temperature
Need complete mechanical properties to make the right choice?
Get complete data on strength, hardness, fatigue, and more.
Free registration required • Instant access
DIN 41 CrMo 4 International Equivalent Materials
Showing 15 of 102 results.
Equivalence categories reflect chemical-composition and mechanical-property comparison — always verify suitability against the governing specification for your application.
Need the full list of 102 international equivalents?
See all 102 equivalent grades with detailed mapping by standard, producer and equivalence category.
Free registration required • Instant access
Optimize material selection for your application - Book A Demo
- 102Cross References
- 7Composition
- 26Mechanical Properties
- 3Physical Properties
- 5Heat Treatment
- 4Metallography
- -Machinability
- -Stress-Strain
- -Formability
- -Fatigue
- -Fracture
- -Creep
- -Joints
- -Coatings
- -Dimensions
- -Tribology
- -Corrosion
- -Ageing
- -Weatherability
- -Irradiation
- 77Total Suppliers