DIN 1.7225 Cast steels
Data updates
This material has 2635 properties — only a subset is shown here.
Unlock full material properties, including detailed values across temperatures and conditions.
Free registration required • Instant access
DIN 1.7225 Chemical Composition
EN 10132-3: 2000 / Cold rolled narrow steel strip for heat treatment - Technical delivery conditions - Part 3: Steels for quenching and tempering
Looking for full material performance data?
Free registration required • Instant access
DIN 1.7225 Physical Properties
Temperature
This material has 2635 properties — only a subset is shown here.
Unlock detailed physical values across temperatures and conditions.
Free registration required • Instant access
DIN 1.7225 Heat Treatments
- (+QT) Quenched: 820-860°C, cooled in oil or water, Tempered: 540-680°C.
- Normalized at 850-880°C
Quenched at 830-860°C
Tempered at 530-670°C
Surface hardened at 820-890°C
DIN 1.7225 Mechanical Properties
Temperature
Need complete mechanical properties to make the right choice?
Get complete data on strength, hardness, fatigue, and more.
Free registration required • Instant access
DIN 1.7225 International Equivalent Materials
Showing 15 of 722 results.
Equivalence categories reflect chemical-composition and mechanical-property comparison — always verify suitability against the governing specification for your application.
Need the full list of 722 international equivalents?
See all 722 equivalent grades with detailed mapping by standard, producer and equivalence category.
Free registration required • Instant access
Optimize material selection for your application - Book A Demo
- 722Cross References
- 167Composition
- 541Mechanical Properties
- 105Physical Properties
- 48Heat Treatment
- 15Metallography
- -Machinability
- 179Stress-Strain
- 71Formability
- 3Fatigue
- -Fracture
- -Creep
- 17Joints
- -Coatings
- 213Dimensions
- -Tribology
- -Corrosion
- -Ageing
- -Weatherability
- -Irradiation
- 554Total Suppliers