DIN GS-42 CrMo 4 Chemical Composition
DIN 17205: 1992 / Quenched and tempered steel castings for general applications; technical delivery conditions
Looking for full material performance data?
Free registration required • Instant access
DIN GS-42 CrMo 4 Heat Treatments
- Air Quenched and Tempered Hardening: 880-950°C; Tempering: 600-650°C Liquid Quenched and Tempered (I) Hardening: 880-950°C; Tempering: 600-650°C Liquid Quenched and Tempered (II) Hardening: 880-950°C; Tempering: 550-600°C
DIN GS-42 CrMo 4 Mechanical Properties
Temperature
Need complete mechanical properties to make the right choice?
Get complete data on strength, hardness, fatigue, and more.
Free registration required • Instant access
DIN GS-42 CrMo 4 International Equivalent Materials
Showing 15 of 622 results.
Equivalence categories reflect chemical-composition and mechanical-property comparison — always verify suitability against the governing specification for your application.
Need the full list of 622 international equivalents?
See all 622 equivalent grades with detailed mapping by standard, producer and equivalence category.
Free registration required • Instant access
Optimize material selection for your application - Book A Demo
- 622Cross References
- 7Composition
- 32Mechanical Properties
- -Physical Properties
- 1Heat Treatment
- -Metallography
- -Machinability
- -Stress-Strain
- -Formability
- 15Fatigue
- -Fracture
- -Creep
- 17Joints
- -Coatings
- -Dimensions
- -Tribology
- -Corrosion
- -Ageing
- -Weatherability
- -Irradiation
- 452Total Suppliers