DIN Ck 60 Structural and constructional steels
Data updates
This material has 1394 properties — only a subset is shown here.
Unlock full material properties, including detailed values across temperatures and conditions.
Free registration required • Instant access
DIN Ck 60 Chemical Composition
DIN 1652-4: 1990 / Bright steel made from steel for quenching and tempering; technical delivery conditions
Looking for full material performance data?
Free registration required • Instant access
DIN Ck 60 Physical Properties
Temperature
This material has 1394 properties — only a subset is shown here.
Unlock detailed physical values across temperatures and conditions.
Free registration required • Instant access
DIN Ck 60 Heat Treatments
- Annealing: 650-700°C; Normalizing: 830-860°C; Hardening in water: 805-835°C; Hardening in oil: 815-845°C; Tempering: 540-680°C
- Hot working: 1050-850°C; Soft annealing: 650-700°C; Normalizing: 820-850°C; Hardening in water: 800-830°C; Hardening in oil: 810-840°C; Tempering: 550-660°C
DIN Ck 60 Mechanical Properties
Temperature
Need complete mechanical properties to make the right choice?
Get complete data on strength, hardness, fatigue, and more.
Free registration required • Instant access
Optimize material selection for your application - Book a Demo
-
676 Cross References
-
25 Composition
-
166 Mechanical Properties
-
3 Physical Properties
-
6 Heat Treatment
-
- Metallography
-
- Machinability
-
- Stress-Strain
-
1 Formability
-
10 Fatigue
-
- Fracture
-
- Creep
-
- Joints
-
- Coatings
-
- Dimensions
-
- Tribology
-
- Corrosion
-
- Ageing
-
- Weatherability
-
- Irradiation
-
507 Total Suppliers