DIN 1.1211 Structural and constructional steels

Material group: Ferrous Alloys / Structural and constructional steels
Country/Standard: Germany / DIN

Data updates

Latest Update: 2022-08
Total number of updates: 2
Update History
2021-12

This material has 699 properties — only a subset is shown here.

Unlock full material properties, including detailed values across temperatures and conditions.

View Complete Material Data ›
Free registration required • Instant access

Free registration required • Instant access

DIN 1.1211 Chemical Composition

CRITERIA
VALUE
UNIT
CAS NUMBER
CRITERIA
C
VALUE
0.7000 – 1.0000
UNIT
%
CAS NUMBER
7440-44-0
CRITERIA
Cu
VALUE
≤ 0.1200
UNIT
%
CAS NUMBER
7440-50-8
CRITERIA
Mn
VALUE
0.3000 – 1.5000
UNIT
%
CAS NUMBER
7439-96-5
CRITERIA
P
VALUE
val1
Full data available with free access View Complete Material Data
UNIT
%
CAS NUMBER
7723-14-0
CRITERIA
S
VALUE
val1
Full data available with free access View Complete Material Data
UNIT
%
CAS NUMBER
7704-34-9
CRITERIA
Si
VALUE
val1
Full data available with free access View Complete Material Data
UNIT
%
CAS NUMBER
7440-21-3

Round steel wire for springs; patented cold drawn, carbon steel wire for springs; technical delivery conditions, DIN 17223-1

Looking for full material performance data?

View Complete Material Data ›
Free registration required • Instant access

Free registration required • Instant access

DIN 1.1211 Physical Properties


Temperature

PROPERTY / VALUE
Modulus of Elasticity
190 — 210 GPa
Unlock full details
Full data available with free access View Complete Material Data
Density
7.67 — 7.86 kg/dm³
Unlock full details
Full data available with free access View Complete Material Data
Poisson Coefficient
0.27 — 0.3
Unlock full details
Full data available with free access View Complete Material Data

This material has 699 properties — only a subset is shown here.

Unlock detailed physical values across temperatures and conditions.

View Complete Material Data ›
Free registration required • Instant access

Free registration required • Instant access

DIN 1.1211 Heat Treatments

  • Austenitizing: 825-855°C, cooling in oil.
  • Austenitized at 800-840°C, quenched in oil or water.

DIN 1.1211 Mechanical Properties


Temperature

PROPERTY / VALUE
Yield Strength, Rp0.2
≤ 495 MPa
Unlock full details
Full data available with free access View Complete Material Data
Tensile Strength
620 MPa
Unlock full details
Full data available with free access View Complete Material Data
Elongation, A
17 %
Unlock full details
Full data available with free access View Complete Material Data
Rockwell Hardness (HR)
val1
Full data available with free access View Complete Material Data
Unlock full details
Full data available with free access View Complete Material Data
Vickers Hardness (HV)
val1
Full data available with free access View Complete Material Data
Unlock full details
Full data available with free access View Complete Material Data

Need complete mechanical properties to make the right choice?

Get complete data on strength, hardness, fatigue, and more.

View Complete Material Data ›
Free registration required • Instant access

Free registration required • Instant access

Book A Demo

Optimize material selection for your application - Book a Demo

  • 337 Cross References

  • 24 Composition
  • 100 Mechanical Properties
  • 3 Physical Properties
  • 5 Heat Treatment
  • - Metallography
  • - Machinability

  • - Stress-Strain
  • - Formability
  • - Fatigue
  • - Fracture
  • - Creep

  • - Joints
  • - Coatings
  • - Dimensions
  • - Tribology

  • - Corrosion
  • - Ageing
  • - Weatherability
  • - Irradiation

  • 230 Total Suppliers