DIN 1.8882 Structural and constructional steels
Data updates
This material has 159 properties — only a subset is shown here.
Unlock full material properties, including detailed values across temperatures and conditions.
Free registration required • Instant access
DIN 1.8882 Chemical Composition
SEW 028: 1993 / Non-alloy and alloy steels with specified properties at moderately elevated and elevated temperatures for pressure vessel purposes; Technical delivery conditions for flat products
Looking for full material performance data?
Free registration required • Instant access
DIN 1.8882 Physical Properties
Temperature
This material has 159 properties — only a subset is shown here.
Unlock detailed physical values across temperatures and conditions.
Free registration required • Instant access
DIN 1.8882 Heat Treatments
- Normalized: 950 to 980°C, after reaching the temperature through out the cross-section cooling in still air; Heat treatment after welding - stress relieved: 530 to 580°C, >= 15min for t <= 15mm, >= 30min for 15 < t <= 30mm, 60min for t > 30mm, cooling in still air.
- Normalized: 950 to 980°C, after reaching the temperature through out the cross-section cooling in still air; Heat treatment after welding - stress relieved: 530 to 580°C, >= 15min for t <= 15mm, >= 30min for 15 < t <= 30mm, 60min for t > 30mm, cooling in still air.
DIN 1.8882 Mechanical Properties
Temperature
Need complete mechanical properties to make the right choice?
Get complete data on strength, hardness, fatigue, and more.
Free registration required • Instant access
Optimize material selection for your application - Book a Demo
-
51 Cross References
-
21 Composition
-
74 Mechanical Properties
-
3 Physical Properties
-
2 Heat Treatment
-
- Metallography
-
- Machinability
-
- Stress-Strain
-
- Formability
-
- Fatigue
-
- Fracture
-
- Creep
-
- Joints
-
- Coatings
-
- Dimensions
-
- Tribology
-
- Corrosion
-
- Ageing
-
- Weatherability
-
- Irradiation
-
8 Total Suppliers