42CrMoS4 (European Union / EN) Material Properties
Other designations:
Material group:
Ferrous Alloys / Structural and constructional steels
Country/Standard:
European Union / EN
Data updates
Latest Update: 2024-12
Total number of updates: 6
Update History:
2019-06
2018-09
2018-08
2018-01
2017-08
Mechanical Properties
Temperature
Physical Properties
Temperature
Coefficient of Thermal Expansion (CTE)
val1
Full data access requires a free trial.
Sign Up Free
10-6/°C
view details
Coefficient of Thermal Expansion (CTE)
val1
Full data access requires a free trial.
Sign Up Free
10-6/°C
view details
Coefficient of Thermal Expansion (CTE)
val1
Full data access requires a free trial.
Sign Up Free
10-6/°C
view details
Thermal Conductivity
val1
Full data access requires a free trial.
Sign Up Free
W/(m∙°C)
view details
Thermal Conductivity
val1
Full data access requires a free trial.
Sign Up Free
W/(m∙°C)
view details
Coefficient of Thermal Expansion (CTE)
val1
Full data access requires a free trial.
Sign Up Free
10-6/°F
view details
Coefficient of Thermal Expansion (CTE)
val1
Full data access requires a free trial.
Sign Up Free
10-6/°F
view details
Coefficient of Thermal Expansion (CTE)
val1
Full data access requires a free trial.
Sign Up Free
10-6/°F
view details
Thermal Conductivity
val1
Full data access requires a free trial.
Sign Up Free
BTU/(h∙ft∙°F)
view details
Thermal Conductivity
val1
Full data access requires a free trial.
Sign Up Free
BTU/(h∙ft∙°F)
view details
Composition
CRITERIA
VALUE
UNIT
CAS NUMBER
CRITERIA
C
VALUE
0.38 – 0.45
UNIT
%
CAS NUMBER
7440-44-0
CRITERIA
Cr
VALUE
0.90 – 1.20
UNIT
%
CAS NUMBER
7440-47-3
CRITERIA
Mn
VALUE
0.60 – 0.90
UNIT
%
CAS NUMBER
7439-96-5
CRITERIA
Mo
VALUE
val1
Full data access requires a free trial.
Sign Up Free
UNIT
%
CAS NUMBER
7439-98-7
CRITERIA
P
VALUE
val1
Full data access requires a free trial.
Sign Up Free
UNIT
%
CAS NUMBER
7723-14-0
CRITERIA
S
VALUE
val1
Full data access requires a free trial.
Sign Up Free
UNIT
%
CAS NUMBER
7704-34-9
CRITERIA
Si
VALUE
val1
Full data access requires a free trial.
Sign Up Free
UNIT
%
CAS NUMBER
7440-21-3
EN 10083-1: 1991 / Quenched and tempered steels - Part 1: Technical delivery conditions for special steels (includes amendment A1:1996)
Heat Treatments
- Austenitizing (quenching in oil or water): 820-880°C, (at least 30 min). NOTE: The temperatures at the lower end of the range are generally applicable to hardening in water and those at the upper end for hardening in oil. Synthetic quenchants may also be used; Tempering: 540-680°C, (at least 60 min); End quench test: 850±5°C.
- Austenitizing (quenching in water or oil): 820-860°C, t > 30 min. NOTE: The temperatures at the lower end of the range are generally applicable to hardening in water and those at the upper end for hardening in oil. Synthetic quenchants may also be used. Tempering: 540-680°C, t > 60 min. A mandatory end quench test shall be carried out at 850+/- 5°C.
-
450 Cross References
-
53 Composition
-
201 Mechanical Properties
-
28 Physical Properties
-
13 Heat Treatment
-
- Metallography
-
- Machinability
-
38 Stress-Strain
-
- Formability
-
5 Fatigue
-
- Fracture
-
- Creep
-
- Joints
-
- Coatings
-
46 Dimensions
-
- Tribology
-
- Corrosion
-
- Ageing
-
- Weatherability
-
- Irradiation
-
276 Total Suppliers