WL 1.1174 Structural and constructional steels
Data updates
This material has 504 properties — only a subset is shown here.
Unlock full material properties, including detailed values across temperatures and conditions.
Free registration required • Instant access
WL 1.1174 Chemical Composition
WL 1.1174: 1978 / Unalloyed heat-treatable steel with about 0.35C; rods and forgings
Looking for full material performance data?
Free registration required • Instant access
WL 1.1174 Physical Properties
Temperature
This material has 504 properties — only a subset is shown here.
Unlock detailed physical values across temperatures and conditions.
Free registration required • Instant access
WL 1.1174 Heat Treatments
- Hot forming at 1150-850°C
- Soft annealed at 650-700°C
Heated at 840-880°C, water or oil quenched, tempered at 550-660°C
WL 1.1174 Mechanical Properties
Temperature
Need complete mechanical properties to make the right choice?
Get complete data on strength, hardness, fatigue, and more.
Free registration required • Instant access
WL 1.1174 International Equivalent Materials
Showing 15 of 265 results.
Equivalence categories reflect chemical-composition and mechanical-property comparison — always verify suitability against the governing specification for your application.
Need the full list of 265 international equivalents?
See all 265 equivalent grades with detailed mapping by standard, producer and equivalence category.
Free registration required • Instant access
Optimize material selection for your application - Book A Demo
- 265Cross References
- 5Composition
- 55Mechanical Properties
- 16Physical Properties
- 2Heat Treatment
- -Metallography
- -Machinability
- 6Stress-Strain
- -Formability
- -Fatigue
- -Fracture
- -Creep
- -Joints
- -Coatings
- -Dimensions
- -Tribology
- -Corrosion
- -Ageing
- -Weatherability
- -Irradiation
- 155Total Suppliers