B.S. TA 11 Titanium Alloys
Data updates
This material has 4384 properties — only a subset is shown here.
Unlock full material properties, including detailed values across temperatures and conditions.
Free registration required • Instant access
B.S. TA 11 Chemical Composition
BS 3TA 11: 2009 / Specification for bar and section for machining of titanium-aluminium-vanadium alloy (tensile strength 900-1160 MPa) (limiting ruling section 150 mm)
Looking for full material performance data?
Free registration required • Instant access
B.S. TA 11 Physical Properties
Temperature
This material has 4384 properties — only a subset is shown here.
Unlock detailed physical values across temperatures and conditions.
Free registration required • Instant access
B.S. TA 11 Heat Treatments
- Annealed + centreless ground or machined (U): 700°C <= θ <= 800°C/t >= 1h/AC or FC (Selected temperature shall be held at ±10°C).
B.S. TA 11 Mechanical Properties
Temperature
Need complete mechanical properties to make the right choice?
Get complete data on strength, hardness, fatigue, and more.
Free registration required • Instant access
B.S. TA 11 International Equivalent Materials
Showing 15 of 36 results.
Equivalence categories reflect chemical-composition and mechanical-property comparison — always verify suitability against the governing specification for your application.
Need the full list of 36 international equivalents?
See all 36 equivalent grades with detailed mapping by standard, producer and equivalence category.
Free registration required • Instant access
Optimize material selection for your application - Book A Demo
- 36Cross References
- 11Composition
- 4Mechanical Properties
- 32Physical Properties
- 1Heat Treatment
- -Metallography
- -Machinability
- 1Stress-Strain
- -Formability
- -Fatigue
- 6Fracture
- -Creep
- -Joints
- -Coatings
- -Dimensions
- -Tribology
- 4283Corrosion
- -Ageing
- -Weatherability
- -Irradiation
- 10Total Suppliers