AISI 348 Physical Properties
Temperature
This material has 254 properties — only a subset is shown here.
Unlock detailed physical values across temperatures and conditions.
Free registration required • Instant access
AISI 348 Heat Treatments
- Annealing: Heating to 982-1121°C (1800-2050°F); air cooling or water quenching. When stress relieving after welding is specified hold for 0.5 hour minimum at 982-1121°C (1800-2050°F) or at 899 ± 13.9°C (1650 ± 25°F) for 2 hours.
AISI 348 International Equivalent Materials
Showing 15 of 150 results.
Equivalence categories reflect chemical-composition and mechanical-property comparison — always verify suitability against the governing specification for your application.
Need the full list of 150 international equivalents?
See all 150 equivalent grades with detailed mapping by standard, producer and equivalence category.
Free registration required • Instant access
Optimize material selection for your application - Book A Demo
- 150Cross References
- -Composition
- -Mechanical Properties
- 3Physical Properties
- 1Heat Treatment
- -Metallography
- -Machinability
- -Stress-Strain
- -Formability
- 1Fatigue
- -Fracture
- -Creep
- 1Joints
- -Coatings
- -Dimensions
- -Tribology
- -Corrosion
- -Ageing
- -Weatherability
- -Irradiation
- 98Total Suppliers