23Mn6 (European Union / EN) Material Properties

Material group: Ferrous Alloys / Structural and constructional steels
Country/Standard: European Union / EN

Data updates

Latest Update: 2018-10
Total number of updates: 1
Update History:

Mechanical Properties


Temperature

0 - 30°C
PROPERTY / VALUE
Yield Strength, Rp0.2 400 MPa view details
Tensile Strength 600 — 850 MPa view details
Elongation, A 15 % view details
Impact Energy val1
Full data access requires a free trial. Sign Up Free
J
view details
Yield Strength, Rp0.2 58 ksi view details
Tensile Strength 87 — 123.3 ksi view details
Elongation, A 15 % view details
Impact Energy val1
Full data access requires a free trial. Sign Up Free
ft·lb
view details

Physical Properties


Temperature

0 - 30°C
PROPERTY / VALUE
Modulus of Elasticity 190 — 210 GPa view details
Density 7.67 — 7.86 kg/dm³ view details
Poisson Coefficient 0.27 — 0.3 view details
Modulus of Elasticity 27.6 E+03 — 30.5 E+03 ksi view details
Density 0.277 — 0.284 lb/in³ view details
Poisson Coefficient 0.27 — 0.3 view details

Composition

CRITERIA
VALUE
UNIT
CAS NUMBER
CRITERIA
C
VALUE
0.19 – 0.26
UNIT
%
CAS NUMBER
7440-44-0
CRITERIA
Cr
VALUE
≤ 0.40
UNIT
%
CAS NUMBER
7440-47-3
CRITERIA
Cr+Mo+Ni
VALUE
≤ 0.63
UNIT
%
CAS NUMBER
CRITERIA
Cu
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7440-50-8
CRITERIA
Mn
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7439-96-5
CRITERIA
Mo
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7439-98-7
CRITERIA
Ni
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7440-02-0
CRITERIA
P
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7723-14-0
CRITERIA
S
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7704-34-9
CRITERIA
Si
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7440-21-3

EN ISO 683-1: 2018 / Heat-treatable steels, alloy steels and free-cutting steels - Part 1: Non-alloy steels for quenching and tempering

Heat Treatments

  • <b> Hardening: </b> 840-900°C (Temperatures at the lower end of the range are generally used for water, and those at the upper end for oil quenching; Time for austenitizing as a guide: at least 30 min.); <br> <b> Quenching agent: </b> Water (Other quenching agents such as synthetic quenchants may also be used.); <br> <b> Tempering: </b> 550-650°C (Time for tempering as a guide: at least 1h.); <br> <b> End quench test austenitizing: </b> 880 ± 5°C (Time for austenitizing as a guide: 30-35 min.).