PROPRIETARY SIQUAL 7227 Structural and constructional steels
Data updates
This material has 314 properties — only a subset is shown here.
Unlock full material properties, including detailed values across temperatures and conditions.
Free registration required • Instant access
PROPRIETARY SIQUAL 7227 Chemical Composition
SIJ - Slovenian Steel Group, Product Data Sheets,
Looking for full material performance data?
Free registration required • Instant access
PROPRIETARY SIQUAL 7227 Physical Properties
Temperature
This material has 314 properties — only a subset is shown here.
Unlock detailed physical values across temperatures and conditions.
Free registration required • Instant access
PROPRIETARY SIQUAL 7227 Heat Treatments
- Soft Annealing: Heat to 680 - 720°C, cool slowly in furnace. Normalizing: 840 - 880°C. Hardening: Harden from a temperature of 820 - 860°C followed by oil or water quenching. Tempering: 540 - 680°C.
PROPRIETARY SIQUAL 7227 Mechanical Properties
Temperature
Need complete mechanical properties to make the right choice?
Get complete data on strength, hardness, fatigue, and more.
Free registration required • Instant access
PROPRIETARY SIQUAL 7227 International Equivalent Materials
Showing 15 of 150 results.
Equivalence categories reflect chemical-composition and mechanical-property comparison — always verify suitability against the governing specification for your application.
Need the full list of 150 international equivalents?
See all 150 equivalent grades with detailed mapping by standard, producer and equivalence category.
Free registration required • Instant access
Optimize material selection for your application - Book A Demo
- 150Cross References
- 5Composition
- 26Mechanical Properties
- 5Physical Properties
- 2Heat Treatment
- -Metallography
- -Machinability
- 5Stress-Strain
- -Formability
- -Fatigue
- -Fracture
- -Creep
- -Joints
- -Coatings
- -Dimensions
- -Tribology
- -Corrosion
- -Ageing
- -Weatherability
- -Irradiation
- 121Total Suppliers