ASME 1.6217 Structural and constructional steels
Data updates
This material has 122 properties — only a subset is shown here.
Unlock full material properties, including detailed values across temperatures and conditions.
Free registration required • Instant access
ASME 1.6217 Chemical Composition
Flat products made of steels for pressure purposes - Part 4: nickel alloy steels with specified low temperature properties, EN 10028-4, 2017
Looking for full material performance data?
Free registration required • Instant access
ASME 1.6217 Physical Properties
Temperature
This material has 122 properties — only a subset is shown here.
Unlock detailed physical values across temperatures and conditions.
Free registration required • Instant access
ASME 1.6217 Heat Treatments
- Normalized (+N) or Normalized and tempered (+NT):
Austenitizing at 880 to 940°C, air cooling.
Tempering at 580 to 640°C, air cooling.
ASME 1.6217 Mechanical Properties
Temperature
Need complete mechanical properties to make the right choice?
Get complete data on strength, hardness, fatigue, and more.
Free registration required • Instant access
ASME 1.6217 International Equivalent Materials
Showing 15 of 48 results.
Equivalence categories reflect chemical-composition and mechanical-property comparison — always verify suitability against the governing specification for your application.
Need the full list of 48 international equivalents?
See all 48 equivalent grades with detailed mapping by standard, producer and equivalence category.
Free registration required • Instant access
Optimize material selection for your application - Book A Demo
- 48Cross References
- 10Composition
- 19Mechanical Properties
- 3Physical Properties
- 1Heat Treatment
- -Metallography
- -Machinability
- -Stress-Strain
- -Formability
- -Fatigue
- -Fracture
- -Creep
- -Joints
- -Coatings
- -Dimensions
- -Tribology
- -Corrosion
- -Ageing
- -Weatherability
- -Irradiation
- 41Total Suppliers