1.6217 (Germany / DIN) Material Properties
Other designations:
,
Material group:
Ferrous Alloys / Structural and constructional steels
Country/Standard:
Germany / DIN
Data updates
Latest Update: 2021-09
Total number of updates: 6
Update History:
2017-09
2017-06
2016-03
2014-05
2014-03
Mechanical Properties
Temperature
Physical Properties
Temperature
Composition
CRITERIA
VALUE
UNIT
CAS NUMBER
CRITERIA
Al
VALUE
≥ 0.020
UNIT
%
CAS NUMBER
7429-90-5
CRITERIA
C
VALUE
≤ 0.16
UNIT
%
CAS NUMBER
7440-44-0
CRITERIA
Cr+Mo+Ni
VALUE
≤ 0.50
UNIT
%
CAS NUMBER
CRITERIA
Mn
VALUE
val1
Full data access requires a free trial.
Sign Up Free
UNIT
%
CAS NUMBER
7439-96-5
CRITERIA
Nb
VALUE
val1
Full data access requires a free trial.
Sign Up Free
UNIT
%
CAS NUMBER
7440-03-1
CRITERIA
Ni
VALUE
val1
Full data access requires a free trial.
Sign Up Free
UNIT
%
CAS NUMBER
7440-02-0
CRITERIA
P
VALUE
val1
Full data access requires a free trial.
Sign Up Free
UNIT
%
CAS NUMBER
7723-14-0
CRITERIA
S
VALUE
val1
Full data access requires a free trial.
Sign Up Free
UNIT
%
CAS NUMBER
7704-34-9
CRITERIA
Si
VALUE
val1
Full data access requires a free trial.
Sign Up Free
UNIT
%
CAS NUMBER
7440-21-3
CRITERIA
V
VALUE
val1
Full data access requires a free trial.
Sign Up Free
UNIT
%
CAS NUMBER
7440-62-2
EN 10028-4: 2017 / Flat products made of steels for pressure purposes - Part 4: nickel alloy steels with specified low temperature properties
Heat Treatments
- (+N) Normalized, (+NT) Normalized and tempered: Austenitized or solution annealed at 880-940°C, cooled in air, Tempered at 580-640°C, cooled in air.
- Hot working: 1050-850°C; Normalizing: 890-940°C; Tempering: 580-640°C; Stress relieving: 520-560°C
-
134 Cross References
-
68 Composition
-
134 Mechanical Properties
-
3 Physical Properties
-
8 Heat Treatment
-
- Metallography
-
- Machinability
-
- Stress-Strain
-
- Formability
-
- Fatigue
-
- Fracture
-
12 Creep
-
108 Joints
-
- Coatings
-
136 Dimensions
-
1 Tribology
-
8491 Corrosion
-
- Ageing
-
- Weatherability
-
- Irradiation
-
126 Total Suppliers