DIN G28Mn6 Cast steels
Data updates
This material has 264 properties — only a subset is shown here.
Unlock full material properties, including detailed values across temperatures and conditions.
Free registration required • Instant access
DIN G28Mn6 Chemical Composition
EN 10293: 2015 / Steel castings for general engineering uses
Looking for full material performance data?
Free registration required • Instant access
DIN G28Mn6 Heat Treatments
- Normalized (+N): 880 to 950°C, cooled in air (for information only);
QT1: Quenched: 880 to 950°C, cooled in liquid (for information only) and tempered from 630 to 680°C;
(+QT2): quenched from 880 to 950°C, cooled in liquid (for information only) and tempered from 580 to 630°C.
DIN G28Mn6 Mechanical Properties
Temperature
Need complete mechanical properties to make the right choice?
Get complete data on strength, hardness, fatigue, and more.
Free registration required • Instant access
DIN G28Mn6 International Equivalent Materials
Showing 15 of 139 results.
Equivalence categories reflect chemical-composition and mechanical-property comparison — always verify suitability against the governing specification for your application.
Need the full list of 139 international equivalents?
See all 139 equivalent grades with detailed mapping by standard, producer and equivalence category.
Free registration required • Instant access
Optimize material selection for your application - Book A Demo
- 139Cross References
- 10Composition
- 12Mechanical Properties
- -Physical Properties
- 1Heat Treatment
- -Metallography
- -Machinability
- -Stress-Strain
- -Formability
- -Fatigue
- -Fracture
- -Creep
- -Joints
- -Coatings
- -Dimensions
- -Tribology
- -Corrosion
- -Ageing
- -Weatherability
- -Irradiation
- 102Total Suppliers