DIN 1.8522 Structural and constructional steels
Data updates
This material has 290 properties — only a subset is shown here.
Unlock full material properties, including detailed values across temperatures and conditions.
Free registration required • Instant access
DIN 1.8522 Chemical Composition
EN 10085: 2001 / Nitriding steels - Technical delivery conditions
Looking for full material performance data?
Free registration required • Instant access
DIN 1.8522 Physical Properties
Temperature
This material has 290 properties — only a subset is shown here.
Unlock detailed physical values across temperatures and conditions.
Free registration required • Instant access
DIN 1.8522 Heat Treatments
- Soft annealing: 680-720°C; Hardening: 870-970°C (0,5 h minimum), oil or water cooling; Tempering: 580-700°C (1 h minimum); Nitriding: 480-570°C.
- Hardened and tempered: heating within range 910-950°C, oil quenching; + heating ≥ 565°C.
DIN 1.8522 Mechanical Properties
Temperature
Need complete mechanical properties to make the right choice?
Get complete data on strength, hardness, fatigue, and more.
Free registration required • Instant access
Optimize material selection for your application - Book a Demo
-
133 Cross References
-
29 Composition
-
26 Mechanical Properties
-
3 Physical Properties
-
7 Heat Treatment
-
4 Metallography
-
- Machinability
-
- Stress-Strain
-
- Formability
-
5 Fatigue
-
- Fracture
-
- Creep
-
- Joints
-
- Coatings
-
- Dimensions
-
- Tribology
-
- Corrosion
-
- Ageing
-
- Weatherability
-
- Irradiation
-
83 Total Suppliers