ASD-STAN 33CrMoV12 Structural and constructional steels
Data updates
This material has 147 properties — only a subset is shown here.
Unlock full material properties, including detailed values across temperatures and conditions.
Free registration required • Instant access
ASD-STAN 33CrMoV12 Chemical Composition
prEN 2763: 1998 / Aerospace series Steel FE-PL1504 (33CrMoV12) Air melted Hardened and tempered Bar for machining De ≤ 80 mm 1200 MPa ≤ Rm ≤ 1350 MPa
Looking for full material performance data?
Free registration required • Instant access
ASD-STAN 33CrMoV12 Physical Properties
Temperature
This material has 147 properties — only a subset is shown here.
Unlock detailed physical values across temperatures and conditions.
Free registration required • Instant access
ASD-STAN 33CrMoV12 Heat Treatments
- Hardened and tempered:
910°C ≤ θ ≤ 950°C / AC or OQ + θ ≥ 565°C / AC - Hardened and tempered:
910°C ≤ θ ≤ 950°C / AC or OQ + θ ≥ 565°C / AC
ASD-STAN 33CrMoV12 Mechanical Properties
Temperature
Need complete mechanical properties to make the right choice?
Get complete data on strength, hardness, fatigue, and more.
Free registration required • Instant access
ASD-STAN 33CrMoV12 International Equivalent Materials
Showing 15 of 64 results.
Equivalence categories reflect chemical-composition and mechanical-property comparison — always verify suitability against the governing specification for your application.
Need the full list of 64 international equivalents?
See all 64 equivalent grades with detailed mapping by standard, producer and equivalence category.
Free registration required • Instant access
Optimize material selection for your application - Book A Demo
- 64Cross References
- 33Composition
- 24Mechanical Properties
- 3Physical Properties
- 3Heat Treatment
- -Metallography
- -Machinability
- -Stress-Strain
- -Formability
- -Fatigue
- -Fracture
- -Creep
- -Joints
- -Coatings
- -Dimensions
- -Tribology
- -Corrosion
- -Ageing
- -Weatherability
- -Irradiation
- 20Total Suppliers