IS 40C8 Structural and constructional steels
Data updates
This material has 557 properties — only a subset is shown here.
Unlock full material properties, including detailed values across temperatures and conditions.
Free registration required • Instant access
IS 40C8 Chemical Composition
IS 5517: 2006 / Steels for Hardening and Tempering - Specification
Looking for full material performance data?
Free registration required • Instant access
IS 40C8 Physical Properties
Temperature
This material has 557 properties — only a subset is shown here.
Unlock detailed physical values across temperatures and conditions.
Free registration required • Instant access
IS 40C8 Heat Treatments
- Annealed: 830-860°C; Subcritical annealed: 650-700°C; Normalized: 830-860°C; Hardened: 830-860°C; Tempered: max. 660°C;
- Hardened and quenched: hardened: 830-860°C, quenched in an oil
IS 40C8 Mechanical Properties
Temperature
Need complete mechanical properties to make the right choice?
Get complete data on strength, hardness, fatigue, and more.
Free registration required • Instant access
IS 40C8 International Equivalent Materials
Showing 15 of 212 results.
Equivalence categories reflect chemical-composition and mechanical-property comparison — always verify suitability against the governing specification for your application.
Need the full list of 212 international equivalents?
See all 212 equivalent grades with detailed mapping by standard, producer and equivalence category.
Free registration required • Instant access
Optimize material selection for your application - Book A Demo
- 212Cross References
- 59Composition
- 76Mechanical Properties
- 4Physical Properties
- 4Heat Treatment
- -Metallography
- -Machinability
- -Stress-Strain
- -Formability
- -Fatigue
- -Fracture
- -Creep
- -Joints
- -Coatings
- 42Dimensions
- -Tribology
- -Corrosion
- -Ageing
- -Weatherability
- -Irradiation
- 160Total Suppliers