SAE D2 Tool steels
Data updates
This material has 469 properties — only a subset is shown here.
Unlock full material properties, including detailed values across temperatures and conditions.
Free registration required • Instant access
SAE D2 Chemical Composition
SAE J 438b: 1970 / Tool and die steels
Looking for full material performance data?
Free registration required • Instant access
SAE D2 Physical Properties
Temperature
This material has 469 properties — only a subset is shown here.
Unlock detailed physical values across temperatures and conditions.
Free registration required • Instant access
SAE D2 Heat Treatments
- Preheated: 650-705°C; hardened and quenched: 982-1024°C, cooling in air. Tempered: 204-370°C. Annealed: 870-900°C, maximum rate of cooling: 22°C/hour.
SAE D2 Mechanical Properties
Temperature
Need complete mechanical properties to make the right choice?
Get complete data on strength, hardness, fatigue, and more.
Free registration required • Instant access
SAE D2 International Equivalent Materials
Showing 15 of 220 results.
Equivalence categories reflect chemical-composition and mechanical-property comparison — always verify suitability against the governing specification for your application.
Need the full list of 220 international equivalents?
See all 220 equivalent grades with detailed mapping by standard, producer and equivalence category.
Free registration required • Instant access
Optimize material selection for your application - Book A Demo
- 220Cross References
- 7Composition
- 3Mechanical Properties
- 3Physical Properties
- 12Heat Treatment
- 12Metallography
- -Machinability
- 1Stress-Strain
- 1Formability
- -Fatigue
- -Fracture
- -Creep
- -Joints
- -Coatings
- -Dimensions
- 13Tribology
- -Corrosion
- -Ageing
- -Weatherability
- -Irradiation
- 197Total Suppliers