UNI X 2 CrNiMo 17 12 Stainless steels
Data updates
This material has 995 properties — only a subset is shown here.
Unlock full material properties, including detailed values across temperatures and conditions.
Free registration required • Instant access
UNI X 2 CrNiMo 17 12 Chemical Composition
UNI 6901: 1971 / Semi-finished products and hot-rolled or forged bars and rods of special alloyed stainless steel, resistant to corrosion and heat
Looking for full material performance data?
Free registration required • Instant access
UNI X 2 CrNiMo 17 12 Physical Properties
Temperature
This material has 995 properties — only a subset is shown here.
Unlock detailed physical values across temperatures and conditions.
Free registration required • Instant access
UNI X 2 CrNiMo 17 12 Heat Treatments
- Forging temperature: 1200-900°C; Quenched and Tempered: 1050-1100°C.
- Material shall be supplied solutionized at 1050 to 1100°C.
UNI X 2 CrNiMo 17 12 Mechanical Properties
Temperature
Need complete mechanical properties to make the right choice?
Get complete data on strength, hardness, fatigue, and more.
Free registration required • Instant access
UNI X 2 CrNiMo 17 12 International Equivalent Materials
Showing 15 of 505 results.
Equivalence categories reflect chemical-composition and mechanical-property comparison — always verify suitability against the governing specification for your application.
Need the full list of 505 international equivalents?
See all 505 equivalent grades with detailed mapping by standard, producer and equivalence category.
Free registration required • Instant access
Optimize material selection for your application - Book A Demo
- 505Cross References
- 40Composition
- 95Mechanical Properties
- 3Physical Properties
- 4Heat Treatment
- -Metallography
- -Machinability
- -Stress-Strain
- -Formability
- -Fatigue
- -Fracture
- -Creep
- -Joints
- -Coatings
- -Dimensions
- -Tribology
- -Corrosion
- -Ageing
- -Weatherability
- -Irradiation
- 348Total Suppliers