DIN X5CrNiMo17-12-2 Stainless steels
Data updates
This material has 3751 properties — only a subset is shown here.
Unlock full material properties, including detailed values across temperatures and conditions.
Free registration required • Instant access
DIN X5CrNiMo17-12-2 Chemical Composition
DIN 1654-5: 1989 / Cold heading and cold extruding steels; technical delivery conditions for stainless steels
Looking for full material performance data?
Free registration required • Instant access
DIN X5CrNiMo17-12-2 Physical Properties
Temperature
This material has 3751 properties — only a subset is shown here.
Unlock detailed physical values across temperatures and conditions.
Free registration required • Instant access
DIN X5CrNiMo17-12-2 Heat Treatments
- (+AT) Solution annealed: 1020-1120°C, cooled sufficiently rapid in air or water.
- Solution annealed (+AT): 1020-1120°C (for guidance only), cooling sufficiently rapid in water or air.
DIN X5CrNiMo17-12-2 Mechanical Properties
Temperature
Need complete mechanical properties to make the right choice?
Get complete data on strength, hardness, fatigue, and more.
Free registration required • Instant access
DIN X5CrNiMo17-12-2 International Equivalent Materials
Showing 15 of 1194 results.
Equivalence categories reflect chemical-composition and mechanical-property comparison — always verify suitability against the governing specification for your application.
Need the full list of 1194 international equivalents?
See all 1194 equivalent grades with detailed mapping by standard, producer and equivalence category.
Free registration required • Instant access
Optimize material selection for your application - Book A Demo
- 1194Cross References
- 276Composition
- 763Mechanical Properties
- 99Physical Properties
- 24Heat Treatment
- 2Metallography
- 1Machinability
- 116Stress-Strain
- 57Formability
- -Fatigue
- -Fracture
- -Creep
- 191Joints
- -Coatings
- 167Dimensions
- -Tribology
- 1Corrosion
- -Ageing
- -Weatherability
- -Irradiation
- 860Total Suppliers