DIN 1.4401 Stainless steels
Data updates
This material has 3965 properties — only a subset is shown here.
Unlock full material properties, including detailed values across temperatures and conditions.
Free registration required • Instant access
DIN 1.4401 Chemical Composition
DIN 1654-5: 1989 / Cold heading and cold extruding steels; technical delivery conditions for stainless steels
Looking for full material performance data?
Free registration required • Instant access
DIN 1.4401 Physical Properties
Temperature
This material has 3965 properties — only a subset is shown here.
Unlock detailed physical values across temperatures and conditions.
Free registration required • Instant access
DIN 1.4401 Heat Treatments
- (+AT) Solution annealed: 1020-1120°C, cooled sufficiently rapid in air or water.
- Solution annealed (+AT): 1020-1120°C (for guidance only), cooling sufficiently rapid in water or air.
DIN 1.4401 Mechanical Properties
Temperature
Need complete mechanical properties to make the right choice?
Get complete data on strength, hardness, fatigue, and more.
Free registration required • Instant access
DIN 1.4401 International Equivalent Materials
Showing 15 of 1287 results.
Equivalence categories reflect chemical-composition and mechanical-property comparison — always verify suitability against the governing specification for your application.
Need the full list of 1287 international equivalents?
See all 1287 equivalent grades with detailed mapping by standard, producer and equivalence category.
Free registration required • Instant access
Optimize material selection for your application - Book A Demo
- 1287Cross References
- 284Composition
- 773Mechanical Properties
- 176Physical Properties
- 24Heat Treatment
- 2Metallography
- 1Machinability
- 116Stress-Strain
- 58Formability
- -Fatigue
- -Fracture
- 1Creep
- 191Joints
- -Coatings
- 164Dimensions
- -Tribology
- 1Corrosion
- -Ageing
- -Weatherability
- -Irradiation
- 887Total Suppliers