Mechanical Properties


Temperature

0 - 30°C
PROPERTY / VALUE
Yield Strength, Rp0.2 val1
Full data access requires a free trial. Sign Up Free
MPa
view details
Tensile Strength 370 — 1270 MPa view details
Elongation, A 8 % view details
Impact Strength val1
Full data access requires a free trial. Sign Up Free
kJ/m²
view details
Impact Energy val1
Full data access requires a free trial. Sign Up Free
J
view details
Brinell Hardness (HB) 107 — 143 view details
Rockwell Hardness (HR) val1
Full data access requires a free trial. Sign Up Free
view details
Yield Strength, Rp0.2 val1
Full data access requires a free trial. Sign Up Free
ksi
view details
Tensile Strength 53.7 — 184.2 ksi view details
Elongation, A 8 % view details
Impact Strength val1
Full data access requires a free trial. Sign Up Free
ft·lb/in²
view details
Impact Energy val1
Full data access requires a free trial. Sign Up Free
ft·lb
view details
Brinell Hardness (HB) 107 — 143 view details
Rockwell Hardness (HR) val1
Full data access requires a free trial. Sign Up Free
view details

Physical Properties


Temperature

0 - 30°C
30 - 100°C
100 - 300°C
≥ 300°C
PROPERTY / VALUE
Modulus of Elasticity 190 — 210 GPa view details
Shear Modulus val1
Full data access requires a free trial. Sign Up Free
GPa
view details
Density val1
Full data access requires a free trial. Sign Up Free
kg/dm³
view details
Poisson Coefficient val1
Full data access requires a free trial. Sign Up Free
view details
Coefficient of Thermal Expansion (CTE) val1
Full data access requires a free trial. Sign Up Free
10-6/°C
view details
Coefficient of Thermal Expansion (CTE) val1
Full data access requires a free trial. Sign Up Free
10-6/°C
view details
Coefficient of Thermal Expansion (CTE) val1
Full data access requires a free trial. Sign Up Free
10-6/°C
view details
Thermal Conductivity 58 W/(m∙°C) view details
Heat Capacity val1
Full data access requires a free trial. Sign Up Free
J/(kg∙°C)
view details
Electrical Resistivity 0.11 Ω∙mm²/m view details
Modulus of Elasticity 27.6 E+03 — 30.5 E+03 ksi view details
Shear Modulus val1
Full data access requires a free trial. Sign Up Free
ksi
view details
Density val1
Full data access requires a free trial. Sign Up Free
lb/in³
view details
Poisson Coefficient val1
Full data access requires a free trial. Sign Up Free
view details
Coefficient of Thermal Expansion (CTE) val1
Full data access requires a free trial. Sign Up Free
10-6/°F
view details
Coefficient of Thermal Expansion (CTE) val1
Full data access requires a free trial. Sign Up Free
10-6/°F
view details
Coefficient of Thermal Expansion (CTE) val1
Full data access requires a free trial. Sign Up Free
10-6/°F
view details
Thermal Conductivity 33.5 BTU/(h∙ft∙°F) view details
Heat Capacity val1
Full data access requires a free trial. Sign Up Free
BTU/(lb∙°F)
view details
Electrical Resistivity 183 E-06 Ω∙circular·mil/ft view details

Composition

CRITERIA
VALUE
UNIT
CAS NUMBER
CRITERIA
C
VALUE
0.16 – 0.22
UNIT
%
CAS NUMBER
7440-44-0
CRITERIA
Mn
VALUE
0.40 – 0.70
UNIT
%
CAS NUMBER
7439-96-5
CRITERIA
P
VALUE
≤ 0.035
UNIT
%
CAS NUMBER
7723-14-0
CRITERIA
S
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7704-34-9
CRITERIA
Si
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7440-21-3

NF A 35-551: 1986 / Case hardening steels - Technical delivery conditions

Heat Treatments

  • <b>Normalization</b> at 875 to 900°C<br> <b>Cementation process</b> at 880 to 930°C <br> <b>Hardening (core)</b> at 870 to 910°C, water quenching <br> <b>Hardening (surface)</b> at 770 to 810°C; water quenching <br> <b>Tempering</b> at 150 to 200°C.
  • <b>Normalized </b> at 875-900°C <br> <b> Heated </b> in the range at 865-895°C, cooled in water and <b>tempered </b> at 550-650°C <br>