AFNOR NF XC 12 Structural and constructional steels
Data updates
This material has 611 properties — only a subset is shown here.
Unlock full material properties, including detailed values across temperatures and conditions.
Free registration required • Instant access
AFNOR NF XC 12 Chemical Composition
NF A 35-551: 1986 / Case hardening steels - Technical delivery conditions
Looking for full material performance data?
Free registration required • Instant access
AFNOR NF XC 12 Physical Properties
Temperature
This material has 611 properties — only a subset is shown here.
Unlock detailed physical values across temperatures and conditions.
Free registration required • Instant access
AFNOR NF XC 12 Heat Treatments
- Normalization at 900 to 925°C
Cementation process at 890 to 940°C
Hardening (core) at 880 to 920°C, water quenching
Hardening (surface) at 770 to 810°C; water quenching
Tempering at 150 to 200°C.
AFNOR NF XC 12 Mechanical Properties
Temperature
Need complete mechanical properties to make the right choice?
Get complete data on strength, hardness, fatigue, and more.
Free registration required • Instant access
AFNOR NF XC 12 International Equivalent Materials
Showing 15 of 312 results.
Equivalence categories reflect chemical-composition and mechanical-property comparison — always verify suitability against the governing specification for your application.
Need the full list of 312 international equivalents?
See all 312 equivalent grades with detailed mapping by standard, producer and equivalence category.
Free registration required • Instant access
Optimize material selection for your application - Book A Demo
- 312Cross References
- 14Composition
- 29Mechanical Properties
- 3Physical Properties
- 1Heat Treatment
- -Metallography
- -Machinability
- -Stress-Strain
- -Formability
- -Fatigue
- -Fracture
- -Creep
- -Joints
- -Coatings
- 2Dimensions
- -Tribology
- -Corrosion
- -Ageing
- -Weatherability
- -Irradiation
- 250Total Suppliers