20MnCr5 (European Union / EN) Material Properties

Other designations:
Material group: Ferrous Alloys / Structural and constructional steels
Country/Standard: European Union / EN

Data updates

Latest Update: 2024-12
Total number of updates: 6
Update History:
2020-12 2019-06 2018-10 2018-08 2017-04

Mechanical Properties


Temperature

0 - 30°C
PROPERTY / VALUE
Yield Strength, Rp0.2 val1
Full data access requires a free trial. Sign Up Free
MPa
view details
Tensile Strength 700 MPa view details
Elongation, A 9.6 — 19.2 % view details
Reduction of Area val1
Full data access requires a free trial. Sign Up Free
%
view details
Impact Energy val1
Full data access requires a free trial. Sign Up Free
J
view details
Brinell Hardness (HB) 140 — 270 view details
Rockwell Hardness (HR) val1
Full data access requires a free trial. Sign Up Free
view details
Grain Size val1
Full data access requires a free trial. Sign Up Free
view details
Yield Strength, Rp0.2 val1
Full data access requires a free trial. Sign Up Free
ksi
view details
Tensile Strength 101.5 ksi view details
Elongation, A 9.6 — 19.2 % view details
Reduction of Area val1
Full data access requires a free trial. Sign Up Free
%
view details
Impact Energy val1
Full data access requires a free trial. Sign Up Free
ft·lb
view details
Brinell Hardness (HB) 140 — 270 view details
Rockwell Hardness (HR) val1
Full data access requires a free trial. Sign Up Free
view details
Grain Size val1
Full data access requires a free trial. Sign Up Free
view details

Physical Properties


Temperature

0 - 30°C
30 - 100°C
100 - 300°C
≥ 300°C
PROPERTY / VALUE
Modulus of Elasticity 80 — 210 GPa view details
Modulus of Elasticity val1
Full data access requires a free trial. Sign Up Free
GPa
view details
Modulus of Elasticity val1
Full data access requires a free trial. Sign Up Free
GPa
view details
Modulus of Elasticity val1
Full data access requires a free trial. Sign Up Free
GPa
view details
Density val1
Full data access requires a free trial. Sign Up Free
kg/dm³
view details
Poisson Coefficient val1
Full data access requires a free trial. Sign Up Free
view details
Coefficient of Thermal Expansion (CTE) val1
Full data access requires a free trial. Sign Up Free
10-6/°C
view details
Coefficient of Thermal Expansion (CTE) val1
Full data access requires a free trial. Sign Up Free
10-6/°C
view details
Coefficient of Thermal Expansion (CTE) val1
Full data access requires a free trial. Sign Up Free
10-6/°C
view details
Thermal Conductivity 41 W/(m∙°C) view details
Heat Capacity val1
Full data access requires a free trial. Sign Up Free
J/(kg∙°C)
view details
Electrical Resistivity 0.16 Ω∙mm²/m view details
Electrical Conductivity val1
Full data access requires a free trial. Sign Up Free
S/m
view details
Modulus of Elasticity 11.6 E+03 — 30.5 E+03 ksi view details
Modulus of Elasticity val1
Full data access requires a free trial. Sign Up Free
ksi
view details
Modulus of Elasticity val1
Full data access requires a free trial. Sign Up Free
ksi
view details
Modulus of Elasticity val1
Full data access requires a free trial. Sign Up Free
ksi
view details
Density val1
Full data access requires a free trial. Sign Up Free
lb/in³
view details
Poisson Coefficient val1
Full data access requires a free trial. Sign Up Free
view details
Coefficient of Thermal Expansion (CTE) val1
Full data access requires a free trial. Sign Up Free
10-6/°F
view details
Coefficient of Thermal Expansion (CTE) val1
Full data access requires a free trial. Sign Up Free
10-6/°F
view details
Coefficient of Thermal Expansion (CTE) val1
Full data access requires a free trial. Sign Up Free
10-6/°F
view details
Thermal Conductivity 23.7 BTU/(h∙ft∙°F) view details
Heat Capacity val1
Full data access requires a free trial. Sign Up Free
BTU/(lb∙°F)
view details
Electrical Resistivity 266 E-06 Ω∙circular·mil/ft view details
Electrical Conductivity val1
Full data access requires a free trial. Sign Up Free
S/in
view details

Composition

CRITERIA
VALUE
UNIT
CAS NUMBER
CRITERIA
C
VALUE
0.17 – 0.22
UNIT
%
CAS NUMBER
7440-44-0
CRITERIA
Cr
VALUE
1.00 – 1.30
UNIT
%
CAS NUMBER
7440-47-3
CRITERIA
Cu
VALUE
≤ 0.40
UNIT
%
CAS NUMBER
7440-50-8
CRITERIA
Mn
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7439-96-5
CRITERIA
P
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7723-14-0
CRITERIA
S
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7704-34-9
CRITERIA
Si
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7440-21-3

EN 10277: 2018 / Bright steel products - Technical delivery conditions

Heat Treatments

  • End quench test austenitizing at 900 ± 5°C (Time for austenitizing as a guide: 30 min minimum);<br><br>Carburizing at 880-980°C (The carburizing temperature depends on the chemical composition of the steel, the mass of the product and the carburizing medium. If the steels are direct hardened, in general, a temperature of 950°C is not exceeded. For special procedures, for example under vacuum, higher temperatures (for example 1020-1050°C) are not unusual);<br><br>Direct and simple hardening at 820-860°C (The kind of quenching agent depends on, for example the shape of the products, the cooling conditions and the amount of furnace filling. If the steels are direct hardened and if there is a danger of distortion, they should be quenched from a temperature between the core-hardening and case-hardening temperatures);<br><br>Double hardening: Core-hardening at 860-900°C and Case-hardening at 780-820°C;<br><br>Tempering at 150-200°C (Time for tempering as a guide: 1h minimum).
  • End quench test: Quench from 870°C Carburizing: 880 to 980°C; NOTE: If steels are direct hardened, in general, a carburizing temperature of 950°C is not exceeded. For special procedures, for example under vacuum, higher temperatures (for example 1020 to 1050°C) are not unusual. Core hardening: 860 to 900°C; Case hardening: 780 to 820°C; Tempering: 150 to 200°C (as a guide, for 1 hour minimum).